摘要
Total hip replacement has been a successful surgical intervention for over 50 years, with the majority of bearings using a polyethylene cup. Long-term failure due to osteolysis and loosening has been widely documented and alternative bearings have been sought. A novel carbon fiber-reinforced poly-ether ether ketone (CFR-PEEK) cup was investigated through experimental friction and wear studies. Friction studies demonstrated the bearings operated in a boundary lubrication condition, with friction factors higher than those for other hip replacement bearings. The wear study was conducted with 36 mm diameter bearings tested against Biolox Delta heads for a period of 10 million cycles. The mean volumetric wear rate was 0.3 mm 3/Mc, indicating the ceramic-on-CFR-PEEK bearing to be a very low wearing option for total hip replacement.
| 源语言 | 英语 |
|---|---|
| 页(从-至) | 1459-1465 |
| 页数 | 7 |
| 期刊 | Journal of Biomedical Materials Research - Part B Applied Biomaterials |
| 卷 | 100 B |
| 期 | 6 |
| DOI | |
| 出版状态 | 已出版 - 8月 2012 |
| 已对外发布 | 是 |
学术指纹
探究 'Wear of ceramic-on-carbon fiber-reinforced poly-ether ether ketone hip replacements' 的科研主题。它们共同构成独一无二的指纹。引用此
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver