跳到主要导航 跳到搜索 跳到主要内容

Uncovering the Intrinsic High Fracture Toughness of Titanium via Lowered Oxygen Impurity Content

  • Xi'an Jiaotong University

科研成果: 期刊稿件 › 文章 › 同行评审

60 引用 (Scopus)

摘要

Titanium (Ti) and its alloys are known to exhibit room-temperature fracture toughness below 130 MPa m1/2, only about one half of the best austenitic stainless steels. It is purported that this is not the best possible fracture resistance of Ti, but a result of oxygen impurities that sensitively retard the activities of plasticity carriers in this hexagonal close-packed metal. By a reduction of oxygen content from the 0.14 wt% in commercial purity Ti to 0.02 wt%, the mode-Ι fracture toughness of the low-oxygen Ti is measured to be as high as KJIc ≈ 255 MPa m1/2, corresponding to J-integral-based crack-initiation toughness of up to JIc ≈ 537 kJ m−2. This extraordinary toughness, reported here for the first time for pure Ti, places Ti among the toughest known materials. The intrinsic high fracture resistance is attributed to the profuse plastic deformation in a significantly enlarged plastic zone, rendered by the pronounced deformation twinning ahead of the crack tip along with ample twin-stimulated 〈c+a〉 dislocation activities, in the absence of impeding oxygen. Controlling the content of a property-controlling impurity thus holds the promise to be a readily applicable strategy to reach for unprecedented damage tolerance in some other structural alloys.

源语言英语
期刊论文编号2408286
期刊Advanced Materials
卷36
期40
DOI
出版状态已出版 - 2 10月 2024

学术指纹

探究 'Uncovering the Intrinsic High Fracture Toughness of Titanium via Lowered Oxygen Impurity Content' 的科研主题。它们共同构成独一无二的学术指纹。

引用此