TY - JOUR
T1 - Tuning the Surface Mn/Al Ratio and Crystal Crystallinity of Mn-Al Oxides by Calcination Temperature for Excellent Acetone Low-Temperature Mineralization
AU - Li, Jian Rong
AU - Zheng, Jie
AU - Wu, Kun
AU - He, Mengmeng
AU - Zhao, Junyi
AU - Meng, Yang
AU - He, Jun
AU - Ren, Hong Yun
AU - Xiao, Hang
AU - He, Chi
N1 - Publisher Copyright:
© 2023 American Chemical Society.
PY - 2023/4/14
Y1 - 2023/4/14
N2 - Here, Mn-Al oxides with the strengthened synergistic effect of Mn and Al species were fabricated by facilely adjusting the calcination temperature with the hydrolysis-driven redox-precipitation method. Results demonstrated that the surface Mn/Al ratio and KMn8O16 phase can be effectively tamed under different calcination temperatures, which obviously alter the CO2 selectivity, reaction rate, and stability of Mn-Al oxides for catalytic oxidation of acetone, among which the Mn5Al-350 catalyst exhibits the best catalytic performance (90% of acetone converted at 159 °C) with CO2 selectivity higher than 99.5%, mainly owing to its higher surface Mn/Al ratio and weaker Mn-O bond with more Mn3+ as compared to Mn5Al-250, Mn5Al-450, and Mn5Al-550. Although a decrease in the consumption rate of acetic acid in the presence of 3.0 vol % H2O leads to the slight reduction of acetone conversion and CO2 yield, Mn5Al-350 still exhibits a superior catalytic stability. The reaction intermediates including acetaldehyde, ethanol, acetic acid, and formic acid species before total mineralization are determined by proton transfer reaction-mass spectrometry, theoretical calculations, and in situ DRIFTS. Theoretical calculations also reveal that the p-orbital interaction of C with a certain anisotropy leads to a weak catalytic effect in the process of acetic acid decomposition as the rate-limiting step.
AB - Here, Mn-Al oxides with the strengthened synergistic effect of Mn and Al species were fabricated by facilely adjusting the calcination temperature with the hydrolysis-driven redox-precipitation method. Results demonstrated that the surface Mn/Al ratio and KMn8O16 phase can be effectively tamed under different calcination temperatures, which obviously alter the CO2 selectivity, reaction rate, and stability of Mn-Al oxides for catalytic oxidation of acetone, among which the Mn5Al-350 catalyst exhibits the best catalytic performance (90% of acetone converted at 159 °C) with CO2 selectivity higher than 99.5%, mainly owing to its higher surface Mn/Al ratio and weaker Mn-O bond with more Mn3+ as compared to Mn5Al-250, Mn5Al-450, and Mn5Al-550. Although a decrease in the consumption rate of acetic acid in the presence of 3.0 vol % H2O leads to the slight reduction of acetone conversion and CO2 yield, Mn5Al-350 still exhibits a superior catalytic stability. The reaction intermediates including acetaldehyde, ethanol, acetic acid, and formic acid species before total mineralization are determined by proton transfer reaction-mass spectrometry, theoretical calculations, and in situ DRIFTS. Theoretical calculations also reveal that the p-orbital interaction of C with a certain anisotropy leads to a weak catalytic effect in the process of acetic acid decomposition as the rate-limiting step.
KW - DFT calculation
KW - Mn−Al oxides
KW - acetone oxidation
KW - calcination temperature
KW - surface property
UR - https://www.scopus.com/pages/publications/85148102312
U2 - 10.1021/acsestengg.2c00331
DO - 10.1021/acsestengg.2c00331
M3 - 文章
AN - SCOPUS:85148102312
SN - 2690-0645
VL - 3
SP - 487
EP - 499
JO - ACS ES and T Engineering
JF - ACS ES and T Engineering
IS - 4
ER -