TY - JOUR
T1 - Stacking-ensemble-learning-based composition regulation and property optimization of A356.2 aluminum alloy
AU - Ma, Ruonan
AU - Tang, Yichuan
AU - Fang, Junxian
AU - He, Yifan
AU - Li, Silong
AU - Liu, Shaopeng
AU - Li, Yue
AU - Fang, Minxia
AU - Huang, Chang
AU - Yang, Sen
AU - Zhang, Yin
N1 - Publisher Copyright:
© 2026 Elsevier Ltd.
PY - 2027/1/1
Y1 - 2027/1/1
N2 - To improve the efficiency of composition optimization for A356.2 aluminum alloy, a literature-derived mechanical-property dataset containing 846 valid modeling records was constructed, including 622 tensile-strength (TS) records and 224 elongation (El) records. Six individual models were first established, and a stacking ensemble learning model (Stacking model) was further developed to predict tensile strength and elongation. The results show that the Stacking model achieved a coefficient of determination ( R 2) of 0.9800 and a mean squared error (MSE) of 44.353 (MPa)2 on the tensile strength test set, and R 2 = 0.7334 and MSE = 0.206 (%)2 on the elongation test set, showing substantially stronger predictive performance for tensile strength than for elongation. SHapley Additive exPlanations (SHAP) analysis ranked Sc as a candidate microalloying element with a potentially positive contribution within the collected dataset. Among the four experimentally investigated alloys, the alloy containing 0.04 wt% Sc exhibited the best overall mechanical properties, with tensile strength and elongation reaching 239 MPa and 7.1%, respectively, corresponding to increases of approximately 25.1% and 65.1% compared with the Sc-free A356.2 base alloy. Microstructural analysis showed that the addition of 0.04 wt% Sc was accompanied by refinement of the α-Al dendritic structure and modification of the eutectic Si morphology. Because no Sc-rich phase was conclusively identified by XRD or SEM-EDS, the observed improvement is primarily associated with the experimentally resolved microstructural changes under the present processing conditions, while any contribution from Sc-containing precipitates remains unconfirmed.
AB - To improve the efficiency of composition optimization for A356.2 aluminum alloy, a literature-derived mechanical-property dataset containing 846 valid modeling records was constructed, including 622 tensile-strength (TS) records and 224 elongation (El) records. Six individual models were first established, and a stacking ensemble learning model (Stacking model) was further developed to predict tensile strength and elongation. The results show that the Stacking model achieved a coefficient of determination ( R 2) of 0.9800 and a mean squared error (MSE) of 44.353 (MPa)2 on the tensile strength test set, and R 2 = 0.7334 and MSE = 0.206 (%)2 on the elongation test set, showing substantially stronger predictive performance for tensile strength than for elongation. SHapley Additive exPlanations (SHAP) analysis ranked Sc as a candidate microalloying element with a potentially positive contribution within the collected dataset. Among the four experimentally investigated alloys, the alloy containing 0.04 wt% Sc exhibited the best overall mechanical properties, with tensile strength and elongation reaching 239 MPa and 7.1%, respectively, corresponding to increases of approximately 25.1% and 65.1% compared with the Sc-free A356.2 base alloy. Microstructural analysis showed that the addition of 0.04 wt% Sc was accompanied by refinement of the α-Al dendritic structure and modification of the eutectic Si morphology. Because no Sc-rich phase was conclusively identified by XRD or SEM-EDS, the observed improvement is primarily associated with the experimentally resolved microstructural changes under the present processing conditions, while any contribution from Sc-containing precipitates remains unconfirmed.
KW - A356.2 aluminum alloy
KW - Mechanical properties
KW - Sc microalloying
KW - SHAP interpretability analysis
KW - Stacking ensemble learning
UR - https://www.scopus.com/pages/publications/105053689437
U2 - 10.1016/j.ssc.2026.116646
DO - 10.1016/j.ssc.2026.116646
M3 - 文章
AN - SCOPUS:105053689437
SN - 0038-1098
VL - 419
JO - Solid State Communications
JF - Solid State Communications
M1 - 116646
ER -