TY - JOUR
T1 - Silicone elastomer dielectric composites by introducing novel O-MMT@TiO2 nanoparticles for energy harvesting application
AU - Yang, Tao
AU - Wang, Chongyang
AU - Liu, Ling
AU - Zhang, Liqun
N1 - Publisher Copyright:
© 2024
PY - 2024/10
Y1 - 2024/10
N2 - Dielectric elastomers have attracted attention in emerging advanced electromechanical applications. However, how to simultaneously improve the dielectric constant and the breakdown strength of dielectric composite needs to be solved. In this paper, we propose a new strategy to anchor TiO2 nanoparticles onto organically modified montmorillonite (O-MMT) nanoplatelets through dehydration reaction to synthesize a novel filler O-MMT@TiO2. Then, the O-MMT@TiO2 is incorporated into methyl vinyl silicone rubber (MVSR) matrix to obtain O-MMT@TiO2/MVSR dielectric composites. Comparing with the composites by direct mixing of TiO2 and O-MMT in MVSR (O-MMT/TiO2/MVSR), O-MMT@TiO2/MVSR composites significantly increase mechanical and dielectric and energy storage properties. 30 wt% O-MMT@TiO2/MVSR composite achieves the highest energy storage density of 118.65 kJ/m3, which is 142.9 % higher than that of 15 wt%O-MMT/15 wt%TiO2/MVSR (48.84 kJ/m3). This study offers an effective method for the preparation of high-performance dielectric elastomer materials, which can be exploited for the energy harvesting application.
AB - Dielectric elastomers have attracted attention in emerging advanced electromechanical applications. However, how to simultaneously improve the dielectric constant and the breakdown strength of dielectric composite needs to be solved. In this paper, we propose a new strategy to anchor TiO2 nanoparticles onto organically modified montmorillonite (O-MMT) nanoplatelets through dehydration reaction to synthesize a novel filler O-MMT@TiO2. Then, the O-MMT@TiO2 is incorporated into methyl vinyl silicone rubber (MVSR) matrix to obtain O-MMT@TiO2/MVSR dielectric composites. Comparing with the composites by direct mixing of TiO2 and O-MMT in MVSR (O-MMT/TiO2/MVSR), O-MMT@TiO2/MVSR composites significantly increase mechanical and dielectric and energy storage properties. 30 wt% O-MMT@TiO2/MVSR composite achieves the highest energy storage density of 118.65 kJ/m3, which is 142.9 % higher than that of 15 wt%O-MMT/15 wt%TiO2/MVSR (48.84 kJ/m3). This study offers an effective method for the preparation of high-performance dielectric elastomer materials, which can be exploited for the energy harvesting application.
KW - Dielectric composites
KW - Energy storage density
KW - O-MMT@TiO nanoparticles
KW - Silicone elastomer
UR - https://www.scopus.com/pages/publications/85198018147
U2 - 10.1016/j.compositesa.2024.108351
DO - 10.1016/j.compositesa.2024.108351
M3 - 文章
AN - SCOPUS:85198018147
SN - 1359-835X
VL - 185
JO - Composites Part A: Applied Science and Manufacturing
JF - Composites Part A: Applied Science and Manufacturing
M1 - 108351
ER -