摘要
Reaction bonded silicon carbide (RB-SiC) was fabricated by phenol resin, starch, solidified agent and silicon powder through the following steps: first, carbonizing at high temperature for 7-9h, infiltrating silicon at 1450-1600°C for 0.5-2H, and then removing excessive silicon at 1700°C for 0.5h. Scanning electron microscopy and X-ray diffraction were employed to characterize and analyze the microstructures and phase composition of the preforms and the final RB-SiC products. In addition, the effect of carbonization temperature, the amount of starch and solidified agent on strength and apparent porosity of final RB-SiC were also discussed. The results showed that the carbonization process of phenol resin can be divided into three steps: at temperatures from 400°C to 600°C, the structure of polymer changes less; at temperatures from 600°C to 1000°C, the fundamental chain of polymer is destroyed, and inverts to glass-like carbon; at temperatures from 1000°C to 1200°C, with the increasing of carbonization temperature, the structure of glass-like carbon changes into the structure of disorder graphite. And the increased micro-pores could be obtained by adding starch.
| 源语言 | 英语 |
|---|---|
| 页(从-至) | 1144-1147 |
| 页数 | 4 |
| 期刊 | Key Engineering Materials |
| 卷 | 336-338 II |
| DOI | |
| 出版状态 | 已出版 - 2007 |
学术指纹
探究 'RB-SiC ceramics derived from the phenol resin added with starch' 的科研主题。它们共同构成独一无二的学术指纹。引用此
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver