TY - JOUR
T1 - Preparation of a silica/poly(n-butyl acrylate-co-acrylic acid) composite latex and its pressure-sensitive properties
AU - Wang, Nongyue
AU - Guo, Yakun
AU - Xu, Hongping
AU - Liu, Xinran
AU - Zhang, Liqun
AU - Qu, Xiongwei
AU - Zhang, Liucheng
PY - 2009/9/5
Y1 - 2009/9/5
N2 - Silica with an average particle size of 125 nm was prepared by the sol-gel reaction of tetraethoxysilane with a base catalyst and then modified with a vinylfunctionalized silane [γ-methacryloxypropyl trimethoxysilane (MPS)]. The composite latex, with the modified silica as the core and poly(n-butyl acrylate-co-acrylic acid) [poly- (BA-co-AA)] polymer as the shell, was synthesized by a semicontinuous emulsion polymerization and used as a pressure-sensitive adhesive. The structures were characterized by Fourier transform infrared spectrometry, X-ray photoelectron spectroscopy, elemental analysis, and transmission electron microscopy. The particle sizes of the silica and MPS-modified silica (MPS-silica)/poly(BA-co-AA) composite latexes were determined by dynamic light scattering in a semicontinuous emulsion polymerization online. The monomers of n-butyl acrylate and acrylic acid grew around the MPS-silica particles without significant secondary nucleation, and the composite latexes exhibited a core-shell structure with the modified silica particles enwrapped in poly(BA-co-AA). To compare the adhesion properties, including the loop tack force, peel strength, and shear resistance, by Fédération Internationale des Fabricants et Transformateurs d'Adhésifs et Thermocollants sur Papiers et Autres Supports test methods, poly(methyl methacrylate-co-allyl methacrylate)/poly(BA-co-AA) latex and the full poly(BA-co-AA) latex were prepared with the same particle size and the same emulsion polymerization process. The shear resistance of the composite latex film greatly increased after the addition of the silica to the core of the poly(BA-co-AA) latex. The relationships between the adhesive properties and the different structures in the core components were examined.
AB - Silica with an average particle size of 125 nm was prepared by the sol-gel reaction of tetraethoxysilane with a base catalyst and then modified with a vinylfunctionalized silane [γ-methacryloxypropyl trimethoxysilane (MPS)]. The composite latex, with the modified silica as the core and poly(n-butyl acrylate-co-acrylic acid) [poly- (BA-co-AA)] polymer as the shell, was synthesized by a semicontinuous emulsion polymerization and used as a pressure-sensitive adhesive. The structures were characterized by Fourier transform infrared spectrometry, X-ray photoelectron spectroscopy, elemental analysis, and transmission electron microscopy. The particle sizes of the silica and MPS-modified silica (MPS-silica)/poly(BA-co-AA) composite latexes were determined by dynamic light scattering in a semicontinuous emulsion polymerization online. The monomers of n-butyl acrylate and acrylic acid grew around the MPS-silica particles without significant secondary nucleation, and the composite latexes exhibited a core-shell structure with the modified silica particles enwrapped in poly(BA-co-AA). To compare the adhesion properties, including the loop tack force, peel strength, and shear resistance, by Fédération Internationale des Fabricants et Transformateurs d'Adhésifs et Thermocollants sur Papiers et Autres Supports test methods, poly(methyl methacrylate-co-allyl methacrylate)/poly(BA-co-AA) latex and the full poly(BA-co-AA) latex were prepared with the same particle size and the same emulsion polymerization process. The shear resistance of the composite latex film greatly increased after the addition of the silica to the core of the poly(BA-co-AA) latex. The relationships between the adhesive properties and the different structures in the core components were examined.
KW - Adhesives
KW - Core-shell polymers
KW - Emulsion polymerization
KW - Silicas
KW - Structure-property relations
UR - https://www.scopus.com/pages/publications/67649990860
U2 - 10.1002/app.30348
DO - 10.1002/app.30348
M3 - 文章
AN - SCOPUS:67649990860
SN - 0021-8995
VL - 113
SP - 3113
EP - 3124
JO - Journal of Applied Polymer Science
JF - Journal of Applied Polymer Science
IS - 5
ER -