N2 - The Ti2AlNb alloys suffer from intrinsic brittleness, which creates a persistent trade-off between strength and ductility at room temperature, and also exhibit insufficient high-temperature strength. To address these limitations, we designed a Ti-22Al-25Nb-1Mo-1Zr-0.25Si (at.%) alloy with a controlled near-equiaxed microstructure consisting of the B2 matrix and O precipitates. The B2/O interface with a lattice mismatch of ∼0.021 facilitates dislocation slip transfer and delays crack initiation. The multi-element co-addition of Mo, Zr and Si refines the grain size, reduces the hardness mismatch between the two phases, and provides sustained solid-solution strengthening. These synergistic effects enable the alloy to achieve a yield strength of approximately 1273 MPa and a fracture elongation of about 11.8% at room temperature, substantially outperforming conventional Ti2AlNb alloys. Remarkably, at 650 °C and 750 °C, the designed alloy retains high yield strengths of about 940 and 732 MPa, with ultimate tensile strengths of about 986 and 873 MPa, respectively. Our findings offer a pathway to overcome the strength-ductility paradox in Ti2AlNb alloys through grain boundary engineering and microstructural control.
AB - The Ti2AlNb alloys suffer from intrinsic brittleness, which creates a persistent trade-off between strength and ductility at room temperature, and also exhibit insufficient high-temperature strength. To address these limitations, we designed a Ti-22Al-25Nb-1Mo-1Zr-0.25Si (at.%) alloy with a controlled near-equiaxed microstructure consisting of the B2 matrix and O precipitates. The B2/O interface with a lattice mismatch of ∼0.021 facilitates dislocation slip transfer and delays crack initiation. The multi-element co-addition of Mo, Zr and Si refines the grain size, reduces the hardness mismatch between the two phases, and provides sustained solid-solution strengthening. These synergistic effects enable the alloy to achieve a yield strength of approximately 1273 MPa and a fracture elongation of about 11.8% at room temperature, substantially outperforming conventional Ti2AlNb alloys. Remarkably, at 650 °C and 750 °C, the designed alloy retains high yield strengths of about 940 and 732 MPa, with ultimate tensile strengths of about 986 and 873 MPa, respectively. Our findings offer a pathway to overcome the strength-ductility paradox in Ti2AlNb alloys through grain boundary engineering and microstructural control.
KW - Deformation mechanisms
KW - Interfaces
KW - Mechanical properties
KW - TiAlNb
UR - https://www.scopus.com/pages/publications/105054858060
U2 - 10.1016/j.actamat.2026.122884
DO - 10.1016/j.actamat.2026.122884
M3 - 文章
AN - SCOPUS:105054858060
SN - 1359-6454
VL - 322
JO - Acta Materialia
JF - Acta Materialia
M1 - 122884
ER -