TY - JOUR
T1 - Microstructure and water-lubricated friction and wear properties of CrN(C) coatings with different carbon contents
AU - Wang, Qianzhi
AU - Zhou, Fei
AU - Ding, Xiangdong
AU - Zhou, Zhifeng
AU - Wang, Chundong
AU - Zhang, Wenjun
AU - Li, Lawrence Kwok Yan
AU - Lee, Shuit Tong
PY - 2013
Y1 - 2013
N2 - The CrN(C) coatings with different carbon contents were deposited using unbalanced magnetron sputtering via adjusting the carbon target current, and their microstructure and mechanical properties were characterized using Raman spectrum, X-ray photoelectron spectroscopy and nano-indenter, respectively. The water-lubricated tribological properties of the CrN(C) coatings against Si 3 N 4 balls were investigated using the ball-on-disk tribometer. The results showed that the C content in the CrN(C) coatings increased gradually, and the peak intensity correlated to Cr 7 C 3 crystal phase became stronger when the carbon target current increased. When the carbon target current was 1 A, the hardness of the CrN(C) coatings increased to 22.5 GPa due to formation of Cr 7 C 3 phase and amorphous CN x , and a little amorphous carbon had positive effect on tribological properties of the CrN(C) coatings in water lubrication. On the other hand, CrN(C) coatings deposited at 2-4 A exhibited a lower hardness and deteriorated tribological properties, due to the presence of a major amount of Cr 2 O 3 particles in the films.
AB - The CrN(C) coatings with different carbon contents were deposited using unbalanced magnetron sputtering via adjusting the carbon target current, and their microstructure and mechanical properties were characterized using Raman spectrum, X-ray photoelectron spectroscopy and nano-indenter, respectively. The water-lubricated tribological properties of the CrN(C) coatings against Si 3 N 4 balls were investigated using the ball-on-disk tribometer. The results showed that the C content in the CrN(C) coatings increased gradually, and the peak intensity correlated to Cr 7 C 3 crystal phase became stronger when the carbon target current increased. When the carbon target current was 1 A, the hardness of the CrN(C) coatings increased to 22.5 GPa due to formation of Cr 7 C 3 phase and amorphous CN x , and a little amorphous carbon had positive effect on tribological properties of the CrN(C) coatings in water lubrication. On the other hand, CrN(C) coatings deposited at 2-4 A exhibited a lower hardness and deteriorated tribological properties, due to the presence of a major amount of Cr 2 O 3 particles in the films.
KW - Mechanical properties
KW - Photoelectron spectroscopy
KW - Sputtering
KW - Thin films
KW - X-ray diffraction
UR - https://www.scopus.com/pages/publications/84875472410
U2 - 10.1016/j.apsusc.2013.01.027
DO - 10.1016/j.apsusc.2013.01.027
M3 - 文章
AN - SCOPUS:84875472410
SN - 0169-4332
VL - 268
SP - 579
EP - 587
JO - Applied Surface Science
JF - Applied Surface Science
ER -