Microstructure and mechanical properties of Y2O3 reinforced Ti6Al4V composites fabricated by spark plasma sintering

  • Ang Li
  • , Shuan Ma
  • , Yanjie Yang
  • , Shiqi Zhou
  • , Lan Shi
  • , Mabao Liu
  • Xi'an Jiaotong University

科研成果: 期刊稿件 › 文章 › 同行评审

55 引用 (Scopus)

摘要

The paper presents the fabrication of (0.6–3.0 wt%) Y2O3-Ti6Al4V composites by spark plasma sintering (SPS) with the sintering heating rate of 100 °C/min and the sintering temperature of 900 °C. Ti6Al4V powders and Y2O3 powders were admixed by rocking mill for 8 h at 30 Hz. Scanning electron microscopy (SEM) equipped with complete energy dispersive spectrometer (EDS) and X-ray diffraction (XRD) were used to characterize the as-received Ti6Al4V powders, Y2O3 powders, the admixed composite powders and the sintered samples. The microhardness, the compressive yield strength and the ultimate strength of as-sintered samples at room temperature were enhanced up to 464.1HV, 1346 MPa and 1583 MPa respectively with a plastic strain of 19.1%, when 2.0 wt% Y2O3 was introduced. The mechanical behaviors of 2.0 wt% Y2O3-Ti6Al4V composite at 450 °C were also carried out with the yield strength of 832 MPa and the ultimate strength of 1088 MPa. Compared with the sintered Ti6Al4V, the 2.0 wt% Y2O3-Ti6Al4V composite has higher yield strength and ultimate strength at elevated temperature with the increment of 54% and 37%, respectively. The mode of fracture was transformed from ductile fracture to a combination of ductile and brittle fractures with the increase of Y2O3 content.

源语言英语
页(从-至)49-56
页数8
期刊Journal of Alloys and Compounds
卷768
DOI
出版状态已出版 - 5 11月 2018