Microstructure and element segregation of Ni-base superalloy casting with radiation and liquid-metal cooling

  • Gang Liu
  • , Lin Liu
  • , Guo Jun Zhang
  • , Jun Zhang
  • Xi'an University of Technology
  • Northwestern Polytechnical University Xian

科研成果: 书/报告/会议事项章节会议稿件同行评审

3 引用 (Scopus)

摘要

A Re-containing single-crystal superalloy was processed with conventional radiation high rate solidification (HRS) and liquid-metal cooling (LMC) techniques, respectively. Compared with the HRS castings, LMC castings exhibited the greatly refined dendrite structures and lower segregation. At the withdrawal rate of 50 μm/s, the primary and secondary dendrite arm spacing of LMC casting was 103 and 19 μm, which were reduced by 60% and 53% compared to the counterpart of HRS castings. Moreover, higher withdrawal rates significantly shortened the characteristic diffusion distance and reduced the residual segregation of refractory elements after homogenization-solution treatments, which is beneficial for improving the local phase stability of Re-containing superalloys.

源语言英语
主期刊名High Performance Structural Material
编辑Yafang Han, Qiang Zhang, Bin Jiang, Bin Jiang
出版商Trans Tech Publications Ltd
608-612
页数5
ISBN(电子版)9783038353959
DOI
出版状态已出版 - 2015
已对外发布
活动Chinese Materials Congress, CMC 2014 - Chengdu, 中国
期限: 4 7月 20147 7月 2014

丛书

姓名Materials Science Forum
816
ISSN(印刷版)0255-5476
ISSN(电子版)1662-9752

会议

会议Chinese Materials Congress, CMC 2014
国家/地区中国
Chengdu
时期4/07/147/07/14

学术指纹

探究 'Microstructure and element segregation of Ni-base superalloy casting with radiation and liquid-metal cooling' 的科研主题。它们共同构成独一无二的学术指纹。

引用此