TY - JOUR
T1 - Mechanistic insights of stage-specific oxidation on tensile behavior of a 4th generation nickel-based single-crystal superalloy
AU - Su, Hao
AU - Cui, Luqing
AU - Cao, Zhenyang
AU - Dang, Xiaofeng
AU - Zhang, Liyin
AU - Zhao, Wang
AU - Li, Yansong
AU - Luo, Sihai
AU - He, Weifeng
AU - Liang, Xiaoqing
N1 - Publisher Copyright:
© 2025 Elsevier Ltd
PY - 2026/1
Y1 - 2026/1
N2 - Under high-temperature service conditions, nickel-based single-crystal superalloys (Ni-SXs) inevitably experience oxidation-assisted surface defect generation and interdiffusion-driven internal matrix alteration, both of which are considered to collectively degrade mechanical performance. However, studies focusing on the independent contributions of stage-specific oxidation behavior to performance evolution remain relatively limited. To address this gap, a Ru-containing fourth-generation SX was selected for oxidation at 1100 ℃ for varying durations, with a detailed analysis of the stage-specific oxidation behavior and its impact on the toughness of the SX. Meanwhile, the relevant oxidation kinetics and product characteristics of each stage were methodically obtained. Interestingly, high-temperature tensile experiments revealed that the multilayer oxides formed during the steady stage significantly enhanced toughness, resulting in an approximately 81 % increase in ductility without compromising strength. In contrast, the early and severely oxidized samples exhibited only a moderate improvement (∼ 6 %) in ductility, accompanied by an ∼ 8 % reduction in strength. Furthermore, through nano-indentation and multiscale characterization, the toughening mechanisms of the gradient-structured oxide layers at the steady stage were primarily attributed to the effective hindrance provided by the dense oxide structures, as well as the (Mo, Re)-rich strip formed by the interlocking of the δ phase and MoO2. During the early and severe oxidation stages, the penetration of matrix by microcracks and reduced effective load-bearing area were considered responsible for the strength degradation, whereas ductility was largely governed by the dispersed oxide particles and Al-rich bilayer, which delayed crack propagation, thereby improving ductility during these stages.
AB - Under high-temperature service conditions, nickel-based single-crystal superalloys (Ni-SXs) inevitably experience oxidation-assisted surface defect generation and interdiffusion-driven internal matrix alteration, both of which are considered to collectively degrade mechanical performance. However, studies focusing on the independent contributions of stage-specific oxidation behavior to performance evolution remain relatively limited. To address this gap, a Ru-containing fourth-generation SX was selected for oxidation at 1100 ℃ for varying durations, with a detailed analysis of the stage-specific oxidation behavior and its impact on the toughness of the SX. Meanwhile, the relevant oxidation kinetics and product characteristics of each stage were methodically obtained. Interestingly, high-temperature tensile experiments revealed that the multilayer oxides formed during the steady stage significantly enhanced toughness, resulting in an approximately 81 % increase in ductility without compromising strength. In contrast, the early and severely oxidized samples exhibited only a moderate improvement (∼ 6 %) in ductility, accompanied by an ∼ 8 % reduction in strength. Furthermore, through nano-indentation and multiscale characterization, the toughening mechanisms of the gradient-structured oxide layers at the steady stage were primarily attributed to the effective hindrance provided by the dense oxide structures, as well as the (Mo, Re)-rich strip formed by the interlocking of the δ phase and MoO2. During the early and severe oxidation stages, the penetration of matrix by microcracks and reduced effective load-bearing area were considered responsible for the strength degradation, whereas ductility was largely governed by the dispersed oxide particles and Al-rich bilayer, which delayed crack propagation, thereby improving ductility during these stages.
KW - High-temperature tensile properties
KW - Nickel-based single-crystal superalloy
KW - Oxide layer toughening mechanism
KW - Stage-specific oxidation behavior
UR - https://www.scopus.com/pages/publications/105019740149
U2 - 10.1016/j.corsci.2025.113431
DO - 10.1016/j.corsci.2025.113431
M3 - 文章
AN - SCOPUS:105019740149
SN - 0010-938X
VL - 258
JO - Corrosion Science
JF - Corrosion Science
M1 - 113431
ER -