Investigation by slow positron beam of defects in CLAM steel induced by helium and hydrogen implantation

  • J. Qiu
  • , Y. Xin
  • , X. Ju
  • , L. P. Guo
  • , B. Y. Wang
  • , Y. R. Zhong
  • , Q. Y. Huang
  • , Y. C. Wu
  • University of Science and Technology Beijing
  • Wuhan University
  • CAS - Institute of High Energy Physics
  • CAS - Institute of Plasma Physics

科研成果: 期刊稿件 › 文章 › 同行评审

43 引用 (Scopus)

摘要

Hydrogen and helium ion beams delivering different doses are used in the ion implantation, at room temperature, of China Low Activation Martensitic (CLAM) steel and the induced defects studied by Doppler broadening of gamma-rays generated in positron annihilation. Defect profiles are analysed in terms of conventional S and W parameters, measures of relative contributions of low and high-momentum electrons in the annihilation peak, as functions of incident positron energies E up to 30 keV. The behaviours of the S-E, W-E and S-W plots under different implantation doses indicate clearly that the induced defect size has obvious variation with depth, taking values that interpolate between surface and bulk values, and depend mainly on helium ion fluences. The S-W plot indicates that two types of defects have formed after ion implantation.

源语言英语
页(从-至)3162-3165
页数4
期刊Nuclear Instruments and Methods in Physics Research, Section B: Beam Interactions with Materials and Atoms
卷267
期18
DOI
出版状态已出版 - 15 9月 2009