TY - JOUR
T1 - In-situ reaction mechanism of Ti3AlC2/TiAl3 composite prepared by powder metallurgy
AU - Gao, Lina
AU - Li, Shufeng
AU - Hui, Dongxu
AU - Wang, Shaodi
AU - Li, Shaolong
AU - Zhang, Xin
AU - Li, Bo
N1 - Publisher Copyright:
© 2025 Elsevier Ltd and Techna Group S.r.l.
PY - 2025/8
Y1 - 2025/8
N2 - The layered MAX phase Ti3AlC2 is an excellent reinforcement for TiAl3 matrix. However, unraveling the complex in-situ reaction mechanism of Ti3AlC2/TiAl3 composites is a challenge of great scientific and practical significance. In this paper, Ti3AlC2/TiAl3 composites were sintered at different temperatures from 630 to 1300 °C by using the TiH2, Al and TiC powder as starting materials via powder metallurgy route. Then the samples were characterized using multiple advanced analytical tools to systematically investigate the in-situ reaction mechanism of the Ti3AlC2/TiAl3 composites. The results indicate that the reinforcement Ti3AlC2 begins to generate at 1100 °C, and a coherent interface relationship is formed between the basal plane of hexagonal Ti3AlC2 phase and TiAl3 matrix. Moreover, this coherent relationship can be inherited into the final Ti3AlC2/TiAl3 composites, which is more conducive to the enhancement of interfacial bonding as well as better transfer of stresses, thus effectively improving the strength and toughness of the composite.
AB - The layered MAX phase Ti3AlC2 is an excellent reinforcement for TiAl3 matrix. However, unraveling the complex in-situ reaction mechanism of Ti3AlC2/TiAl3 composites is a challenge of great scientific and practical significance. In this paper, Ti3AlC2/TiAl3 composites were sintered at different temperatures from 630 to 1300 °C by using the TiH2, Al and TiC powder as starting materials via powder metallurgy route. Then the samples were characterized using multiple advanced analytical tools to systematically investigate the in-situ reaction mechanism of the Ti3AlC2/TiAl3 composites. The results indicate that the reinforcement Ti3AlC2 begins to generate at 1100 °C, and a coherent interface relationship is formed between the basal plane of hexagonal Ti3AlC2 phase and TiAl3 matrix. Moreover, this coherent relationship can be inherited into the final Ti3AlC2/TiAl3 composites, which is more conducive to the enhancement of interfacial bonding as well as better transfer of stresses, thus effectively improving the strength and toughness of the composite.
KW - In-situ reaction mechanism
KW - Interface structure
KW - MAX phase
KW - TiAlC/TiAl composites
UR - https://www.scopus.com/pages/publications/105003806273
U2 - 10.1016/j.ceramint.2025.04.376
DO - 10.1016/j.ceramint.2025.04.376
M3 - 文章
AN - SCOPUS:105003806273
SN - 0272-8842
VL - 51
SP - 31836
EP - 31847
JO - Ceramics International
JF - Ceramics International
IS - 20
ER -