A series of lithium niobate (Mg:Mn:Fe:LiNbO3) crystal doped with 0.03% Fe2O3 and 0.1% MnO2 (in mass) and with different the MgO contents of 0, 1%, 3%, 4.5% and 6% in mole were grown by the Czochralski method from congruent melting. Their infrared spectrum and photodamage resistance ability were measured. The results show that the OH- absorption peak of the Mg (0, 1%, 3%, 4.51%):Mn:Fe:LiNbO3 crystals is at 3484 cm-1, while that of 6% Mg doped Mg:Mn:Fe:LiNbO3 shifts to 3535 cm-1. Holographic storage properties of crystals were measured with He-Ne laser at the wavelength of 632 m by two wave coupling method. The results show that the response time and dynamic range of crystals decrease, but photorefractive sensitivity and photodamage resistance ability improve with the increase of Mg doping concentration in crystals. Mg:Mn:Fe:LiNbO3 crystal with the optimal doping concentration of 3% Mg is suitable for holographic storage medium.
| 源语言 | 英语 |
|---|---|
| 页(从-至) | 1013-1016 |
| 页数 | 4 |
| 期刊 | Kuei Suan Jen Hsueh Pao/ Journal of the Chinese Ceramic Society |
| 卷 | 35 |
| 期 | 8 |
| 出版状态 | 已出版 - 8月 2007 |
| 已对外发布 | 是 |
学术指纹
探究 'Holographic storage properties of Mg:Mn:Fe:LiNbO3 crystals' 的科研主题。它们共同构成独一无二的学术指纹。引用此
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver