跳到主要导航 跳到搜索 跳到主要内容

High-temperature corrosion of water-wall tubes in oxy-combustion atmosphere

  • Qiming Jin
  • , Gaofeng Dai
  • , Yongbing Wang
  • , Zhao Wang
  • , Zhiliang Shan
  • , Xuebin Wang
  • , Lan Zhang
  • , Houzhang Tan
  • , Hrvoje Mikulčić
  • Xi'an Jiaotong University
  • Xinjiang Uygur Autonomous Region Special Equipment Inspection and Research Institute
  • Thermal Power Research Institute
  • Henan Province Boiler Pressure Vessel Safety Inspection Institute

科研成果: 期刊稿件 › 文章 › 同行评审

14 引用 (Scopus)

摘要

Oxy-combustion is one of the most promising technology for CO2 capture in coal-fired power plants. However, under oxy-combustion conditions, the concentrations of acid gas species are significantly increased due to the introduction of the flue gas recycle, which aggravates the high-temperature corrosion of heat exchanger materials in boilers. In this study, the early-stage high-temperature corrosion (0–16 h) of two representative water-wall tube materials (20G, 12Cr1MoV) is experimentally tested in a lab-scale furnace with the simulated oxy-combustion atmosphere. The effects of material, temperature, CO2, H2O, SO2, H2S and CO atmospheres on high-temperature corrosion behaviors is investigated. The micro-morphologies and compositions of corrosion layers are characterized by scanning electron microscope with energy dispersive X-ray spectra (SEM-EDS) and X-ray diffraction (XRD). Kinetic analysis shows that the high concentration of CO2 accelerates high-temperature corrosion of water wall materials. In the simulated oxy-fuel combustion atmosphere (CO2/O2/SO2), the mass gain rate can be enhanced by 10%–30% compared to the conventional air combustion atmosphere (N2/O2/SO2), and the major composition of oxide scale is magnetite. In a reducing oxy-fuel atmosphere (CO2/CO/SO2/H2S), the major components of oxide scale are magnetite and ferrous sulfide. The high concentration of moisture in the atmosphere accelerated the corrosion rate by 10–30%. For both model alloys, the corrosion kinetics obey the parabolic law. Water-wall tube material 12Cr1MoV appears superiority in corrosion resistance compared with 20G material.

源语言英语
页(从-至)1305-1312
页数8
期刊Journal of the Energy Institute
卷93
期4
DOI
出版状态已出版 - 8月 2020

联合国可持续发展目标

此成果有助于实现下列可持续发展目标:

  1. 可持续发展目标 7 - 经济适用的清洁能源
    可持续发展目标 7 经济适用的清洁能源

学术指纹

探究 'High-temperature corrosion of water-wall tubes in oxy-combustion atmosphere' 的科研主题。它们共同构成独一无二的学术指纹。

引用此