N2 - The high-temperature sulfur corrosion resistance of S30432 and TP310HCbN typically used in the superheater and reheater of a 620°C ultra-supercritical boiler is investigated in this study. Samples coated with coal ash are placed in a device filled with simulated flue gas at 650°C and 700°C, respectively, for 2000 h. The samples are then analyzed through X-ray diffraction, scanning electron microscopy, and energy-dispersive spectroscopy. S30432 is mainly oxidized under 650°C and 0.2% SO2 volume concentration, and the weight reduction is 6.6 mg cm−2. However, under 700°C and 0.3% SO2 volume concentration, severe sulfidation reaction occurs, sharply accelerating high-temperature corrosion. As a result, weight reduction up to 41.8 mg cm−2 occurs. Although sulfidation reaction also occurs in TP310HCbN, there is no serious corrosion; the corrosion rate reduces in the later stages of the experiment, and a weight increase of 2.4 mg cm−2 is observed. After 11 520 h of the actual operation of the 1000 MW 620°C boiler, there is no obvious high-temperature corrosion in the high-temperature areas without coke-block adhesion. These results indicate that S30432 and TP310HCbN satisfy the requirements of 620°C ultra-supercritical boilers burning high-sulfur coal.
AB - The high-temperature sulfur corrosion resistance of S30432 and TP310HCbN typically used in the superheater and reheater of a 620°C ultra-supercritical boiler is investigated in this study. Samples coated with coal ash are placed in a device filled with simulated flue gas at 650°C and 700°C, respectively, for 2000 h. The samples are then analyzed through X-ray diffraction, scanning electron microscopy, and energy-dispersive spectroscopy. S30432 is mainly oxidized under 650°C and 0.2% SO2 volume concentration, and the weight reduction is 6.6 mg cm−2. However, under 700°C and 0.3% SO2 volume concentration, severe sulfidation reaction occurs, sharply accelerating high-temperature corrosion. As a result, weight reduction up to 41.8 mg cm−2 occurs. Although sulfidation reaction also occurs in TP310HCbN, there is no serious corrosion; the corrosion rate reduces in the later stages of the experiment, and a weight increase of 2.4 mg cm−2 is observed. After 11 520 h of the actual operation of the 1000 MW 620°C boiler, there is no obvious high-temperature corrosion in the high-temperature areas without coke-block adhesion. These results indicate that S30432 and TP310HCbN satisfy the requirements of 620°C ultra-supercritical boilers burning high-sulfur coal.
KW - 620°C boiler
KW - S30432
KW - TP310HCbN
KW - coal-ash
KW - high-temperature corrosion
UR - https://www.scopus.com/pages/publications/85125388199
U2 - 10.1002/maco.202113014
DO - 10.1002/maco.202113014
M3 - 文章
AN - SCOPUS:85125388199
SN - 0947-5117
VL - 73
SP - 1222
EP - 1235
JO - Materials and Corrosion
JF - Materials and Corrosion
IS - 8
ER -