TY - JOUR
T1 - High energy storage density and efficiency in lead-free dielectric ceramics through compositionally graded systems
AU - Shi, Wenjing
AU - Chen, Fukang
AU - Nie, Xinru
AU - Shur, Vladimir
AU - Jin, Li
N1 - Publisher Copyright:
© 2025 Elsevier B.V.
PY - 2025/8/20
Y1 - 2025/8/20
N2 - Achieving concurrent enhancement of energy storage density and efficiency in lead-free dielectric ceramics remains a central challenge in energy storage research. Here, we report a compositionally graded 0.8[(1–x)Bi0.5Na0.4K0.1TiO3-xSrTiO3]-0.2Bi(Mg0.5Zr0.5)O3-0.5 wt% MnO2 ceramic system, with x ranging from 0.3 to 0.6, designed to realize synergistic modulation of structure and defect chemistry. By integrating SrTiO3-induced relaxor ferroelectric behavior, Bi(Mg0.5Zr0.5)O3-driven structural optimization, and MnO2-mediated oxygen vacancy suppression, we achieve a balanced improvement in polarization strength, breakdown field, and efficiency. X-ray diffraction and Raman spectroscopy confirm that the gradient incorporation of SrTiO3 increases the average A-site ionic radius, promoting a low-angle shift in the perovskite lattice while preserving B–O bond vibrational stability. The B-site mismatch introduced by Bi(Mg0.5Zr0.5)O3 enhances relaxor ferroelectric characteristics and boosts dielectric breakdown strength. Simultaneously, trace MnO2 addition mitigates oxygen vacancy-related losses, effectively reducing remanent polarization and enhancing energy storage efficiency. The optimized composition at 0.8(0.4Bi0.5Na0.4K0.1TiO3-0.6SrTiO3)-0.2Bi(Mg0.5Zr0.5)O3-0.5 wt% MnO2 exhibits an exceptional recoverable energy density (Wrec) of 5.53 J/cm3 and efficiency of 91.5 % under 380 kV/cm. Moreover, it demonstrates ultrafast discharge speed (t0.9=1.5 μs) and excellent thermal stability, with only a 5.7 % loss in Wrec (from 3.5 to 3.3 J/cm3) at 140 °C. These findings offer a new pathway toward the co-optimization of polarization, breakdown field, and efficiency in environmentally benign dielectric energy storage systems.
AB - Achieving concurrent enhancement of energy storage density and efficiency in lead-free dielectric ceramics remains a central challenge in energy storage research. Here, we report a compositionally graded 0.8[(1–x)Bi0.5Na0.4K0.1TiO3-xSrTiO3]-0.2Bi(Mg0.5Zr0.5)O3-0.5 wt% MnO2 ceramic system, with x ranging from 0.3 to 0.6, designed to realize synergistic modulation of structure and defect chemistry. By integrating SrTiO3-induced relaxor ferroelectric behavior, Bi(Mg0.5Zr0.5)O3-driven structural optimization, and MnO2-mediated oxygen vacancy suppression, we achieve a balanced improvement in polarization strength, breakdown field, and efficiency. X-ray diffraction and Raman spectroscopy confirm that the gradient incorporation of SrTiO3 increases the average A-site ionic radius, promoting a low-angle shift in the perovskite lattice while preserving B–O bond vibrational stability. The B-site mismatch introduced by Bi(Mg0.5Zr0.5)O3 enhances relaxor ferroelectric characteristics and boosts dielectric breakdown strength. Simultaneously, trace MnO2 addition mitigates oxygen vacancy-related losses, effectively reducing remanent polarization and enhancing energy storage efficiency. The optimized composition at 0.8(0.4Bi0.5Na0.4K0.1TiO3-0.6SrTiO3)-0.2Bi(Mg0.5Zr0.5)O3-0.5 wt% MnO2 exhibits an exceptional recoverable energy density (Wrec) of 5.53 J/cm3 and efficiency of 91.5 % under 380 kV/cm. Moreover, it demonstrates ultrafast discharge speed (t0.9=1.5 μs) and excellent thermal stability, with only a 5.7 % loss in Wrec (from 3.5 to 3.3 J/cm3) at 140 °C. These findings offer a new pathway toward the co-optimization of polarization, breakdown field, and efficiency in environmentally benign dielectric energy storage systems.
KW - BNKT
KW - BNT-based
KW - Dielectric
KW - Lead-free
KW - MnO-doped
UR - https://www.scopus.com/pages/publications/105012768787
U2 - 10.1016/j.jallcom.2025.182903
DO - 10.1016/j.jallcom.2025.182903
M3 - 文章
AN - SCOPUS:105012768787
SN - 0925-8388
VL - 1038
JO - Journal of Alloys and Compounds
JF - Journal of Alloys and Compounds
M1 - 182903
ER -