Double-sided argon arc welded joint of a titanium ally, which is named as TA15, was treated by laser shock peening (LSP). The hardness, residual stress, fatigue life and the mechanism of fatigue crack nucleation of the joints before and after LSP strengthening were compared and analyzed. The results show that: the surface hardness of the welded joint was increased; the initiation location of fatigue crack was transferred from the surface defect with high stress concentration to the interior. At the stress ratio of 0.1, the high stress level (590 MPa) life was improved by about 4.6 times, and the medium stress level (330 MPa) life was improved by 9.9 times. Murakami model as well as modified Murakami formula was used to evaluate and calculate the fatigue strength of double-side welded TA15 procedures by laser shock peening. The maximum error between the calculated results and the experimental results is 22.6%, and the minimum error is 7.78%.
| 源语言 | 英语 |
|---|---|
| 页(从-至) | 10304-10313 |
| 页数 | 10 |
| 期刊 | Journal of Materials Engineering and Performance |
| 卷 | 31 |
| 期 | 12 |
| DOI | |
| 出版状态 | 已出版 - 12月 2022 |
| 已对外发布 | 是 |
学术指纹
探究 'Fatigue Resistance Improvement on Double-Sided Welded Joints of a Titanium Alloy Treated by Laser Shock Peening' 的科研主题。它们共同构成独一无二的学术指纹。引用此
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver