Biological tissues resist fatigue by possessing high fatigue threshold and extremely slow crack growth above the threshold. In contrast, most synthetic hydrogels rely solely on increasing fatigue thresholds and fracture rapidly once cracks start to propagate. Here, we realize fatigue damage tolerance design (FDT) for hydrogels via the synergy of two kinetically distinct metal-ligand crosslinks. Under cyclic loads, the strong and irreversible crosslinks break to dissipate energy, shielding the weak and reversible crosslinks to re-associate upon unloading. The synergistic kinetic effects between these two crosslinks lead to the formation of a large inelastic zone at the crack tip, deconcentrating stress and significantly decelerating fatigue crack growth. The as-synthesized hydrogel exhibits outstanding fatigue resistance, with a threshold of 680 J/m2 and an ultraslow crack growth of 1.08 mm after 106 cycles under an energy release rate of 1000 J/m2. Remarkably, even at a higher energy release rate of ∼3000 J/m2, the fatigue crack growth rate remains below 10-7 m/cycle. This extremely slow crack growth leads to the anti-fatigue hydrogel with a long lifespan under a broad range of the applied load level. The synergistic design of kinetically distinct metal-ligand crosslinks provides a framework for fatigue-resistant soft materials.

源语言英语
页(从-至)43099-43108
页数10
期刊ACS Applied Materials and Interfaces
卷18
期31
DOI
出版状态已出版 - 12 8月 2026
已对外发布是

学术指纹

探究 'Fatigue Damage-Tolerant Hydrogel Engineered via Synergy of Kinetically Distinct Metal-Ligand Crosslinks' 的科研主题。它们共同构成独一无二的学术指纹。

引用此