摘要
To prepare lead zirconate titanate (Pb(ZrxTi1-x)O3): PZT) thin films at a higher deposition rate and a lower substrate temperature, the PZT films were fabricated by a hybrid process of sol-gel technique and pulsed laser ablation deposition. First, one layer of PZT (about 0.12-0.14 μm) was coated on Si/SiO2/Ti/Pt substrate by sol-gel process. Then PZT film was deposited at a rate of 0.7 μm/hr by pulsed excimer laser-ablation on the substrate with one sol-gel derived PZT seed layer. A target of Pb(Zr0.52Ti0.48)O3 with 20 wt% excess PbO was used. The substrate temperature was about 500 °C. The film fabricated by the hybrid process showed the perovskite PZT phase without pyrochlore phase. The dielectric constant measured at 1 kHz was approximately 1580. The saturation polarization, remnant polarization and coercive field of 0.8 μm thick film were about 46.6 μC/cm2, 24.5 μC/cm2 and 36.4 kV/cm, respectively. The residual stresses in the thin film stacks were measured by the changes in the radius of curvature of the wafer. A relatively lower tensile stress (approximately 33 MPa) was obtained compared to the sol-gel derived PZT film. Therefore, the PZT films with good electrical and mechanical properties can be fabricated by using the hybrid process of the sol-gel technique and laser ablation.
| 源语言 | 英语 |
|---|---|
| 页(从-至) | 30-37 |
| 页数 | 8 |
| 期刊 | Proceedings of SPIE - The International Society for Optical Engineering |
| 卷 | 4934 |
| DOI | |
| 出版状态 | 已出版 - 2002 |
| 已对外发布 | 是 |
| 活动 | Smart Materials II - Melbourne, VIC., 美国 期限: 16 12月 2002 → 18 12月 2002 |
学术指纹
探究 'Electrical and mechanical properties of PZT thin films prepared by hybrid process of Sol-gel technique and laser ablation' 的科研主题。它们共同构成独一无二的学术指纹。引用此
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver