跳到主要导航 跳到搜索 跳到主要内容

Effects of pH on the nano/micro structure of calcium silicate hydrate (C-S-H) under sulfate attack

  • Xin Liu
  • , Pan Feng
  • , Wei Li
  • , Guoqing Geng
  • , Jiale Huang
  • , Yun Gao
  • , Song Mu
  • , Jinxiang Hong
  • Southeast University, Nanjing
  • State Key Laboratory of High Performance Civil Engineering Materials
  • Yangzhou University
  • National University of Singapore
  • Ltd.

科研成果: 期刊稿件文章同行评审

133 引用 (Scopus)

摘要

Calcium silicate hydrate (C-S-H), the most important Portland cement hydration product, determines the mechanical properties and durability of cementitious materials. In marine environment, C-S-H often suffers from sulfate attack – one of the most common and severe degradations for concrete. pH is considered as a critical factor in determining the deterioration behavior of C-S-H during sulfate attack, of which the significance may be overlooked. This study focused on the role of pH on the deterioration of C-S-H in terms of the composition and nano/micro structure under sulfate attack. The results show that lowering pH aggravates the decalcification of C-S-H, whereas a strong alkaline condition is beneficial to increase the resistance to deterioration. An increase in the mean chain length together with the proportion of large pores (>10 nm) is observed when C-S-H is subjected to low-pH sulfate attack (pH = 10–12), resulting in a relatively loose structure. The deep analysis on defective tobermorite model reveals that calcium at the interlayer of C-S-H nanostructure is readily removed under sulfate attack, thereby improving the potential of Si-O-Si groups formation and increases the mean chain length of C-S-H.

源语言英语
文章编号106306
期刊Cement and Concrete Research
140
DOI
出版状态已出版 - 2月 2021
已对外发布

联合国可持续发展目标

此成果有助于实现下列可持续发展目标:

  1. 可持续发展目标 14 - 水下生物
    可持续发展目标 14 水下生物

学术指纹

探究 'Effects of pH on the nano/micro structure of calcium silicate hydrate (C-S-H) under sulfate attack' 的科研主题。它们共同构成独一无二的指纹。

引用此