TY - JOUR
T1 - Effects of (Li0.5Sm0.5)/W co-substitution and sintering temperature on the structure and electrical properties of ultrahigh Curie temperature piezoceramics, Ca0.92(Li0.5Sm0.5)0.08Bi2Nb2-xWxO9
AU - Long, Changbai
AU - Ji, Ning
AU - Yang, Li
AU - Zhou, Wenjie
AU - Zheng, Kun
AU - Ren, Wei
AU - Liu, Laijun
N1 - Publisher Copyright:
© 2021 Elsevier Ltd
PY - 2021/6
Y1 - 2021/6
N2 - With co-substitution of (Li0.5Sm0.5) at A site and W at B site, the electrical properties of modified Ca0.92(Li0.5Sm0.5)0.08Bi2Nb2-xWxO9 [(CLS)BN-xW, x = 0, 0.015 and 0.03] piezoceramics with ultrahigh Curie temperature (TC) of > 930 °C were enhanced dramatically. The increased resistivity induced by the co-substitution ensure them to be polarized under an enough high field. Combined with the increase of spontaneous ferroelectric polarization (PS), the significant enhancements in the piezoelectric, dielectric and ferroelectric properties can be obtained in the composition x = 0.015. Furthermore, the piezoelectric activity (d33) and bulk resistivity (ρb) of (CLS)BN-0.015 W can be further enhanced at an appropriate sintering temperature. This optimum composition sintered at 1170 °C shows ultrahigh TC of ∼948 °C, d33 of ∼17.3 pC/N and ρb of ∼6.9 MΩ cm at 600 °C, which are comparable to those of the reported high-temperature Aurivillius piezoceramics with TC > 850 °C.
AB - With co-substitution of (Li0.5Sm0.5) at A site and W at B site, the electrical properties of modified Ca0.92(Li0.5Sm0.5)0.08Bi2Nb2-xWxO9 [(CLS)BN-xW, x = 0, 0.015 and 0.03] piezoceramics with ultrahigh Curie temperature (TC) of > 930 °C were enhanced dramatically. The increased resistivity induced by the co-substitution ensure them to be polarized under an enough high field. Combined with the increase of spontaneous ferroelectric polarization (PS), the significant enhancements in the piezoelectric, dielectric and ferroelectric properties can be obtained in the composition x = 0.015. Furthermore, the piezoelectric activity (d33) and bulk resistivity (ρb) of (CLS)BN-0.015 W can be further enhanced at an appropriate sintering temperature. This optimum composition sintered at 1170 °C shows ultrahigh TC of ∼948 °C, d33 of ∼17.3 pC/N and ρb of ∼6.9 MΩ cm at 600 °C, which are comparable to those of the reported high-temperature Aurivillius piezoceramics with TC > 850 °C.
KW - (LiSm)/W co-substitution
KW - Aurivillius-phase piezoceramics
KW - Electrical properties
KW - Sintering temperature
KW - Ultrahigh curie temperature
UR - https://www.scopus.com/pages/publications/85100008918
U2 - 10.1016/j.jeurceramsoc.2021.01.028
DO - 10.1016/j.jeurceramsoc.2021.01.028
M3 - 文章
AN - SCOPUS:85100008918
SN - 0955-2219
VL - 41
SP - 3369
EP - 3378
JO - Journal of the European Ceramic Society
JF - Journal of the European Ceramic Society
IS - 6
ER -