N2 - This paper investigates the influence of braiding architectures on the out-of-plane shear performance of three-dimensional Braided Composites (3D BCs). Eight types of 3D BCs—comprising four distinct braiding structures (3D four-directional (3D4d), five-directional (3D5d), six-directional (3D6d), and seven-directional (3D7d)), each fabricated with two braiding angles (20° and 40°)—are experimentally evaluated using the Short Beam Shear (SBS) method. In-situ strain fields during testing are recorded by Digital Image Correlation (DIC), and internal damage mechanisms are identified through micro-Computed Tomography (micro-CT). The results indicate that although the shear strength and energy absorption are jointly influenced by both braiding angle and structure, the specimens with a 20° braiding angle generally demonstrate a higher initial modulus, enhanced failure strength, and improved energy absorption relative to those braided at 40°. The damage mechanisms of 3D BCs have significant differences between the four kinds braiding structures, primarily due to the different orientations of the yarns. Furthermore, progressive damage analysis of the 3D BCs specimen reveals that matrix cracking is the initial damage pattern, followed by crack propagation along the braiding yarns and ultimate failure occurs as fiber fracture at the bottom of the specimen.
AB - This paper investigates the influence of braiding architectures on the out-of-plane shear performance of three-dimensional Braided Composites (3D BCs). Eight types of 3D BCs—comprising four distinct braiding structures (3D four-directional (3D4d), five-directional (3D5d), six-directional (3D6d), and seven-directional (3D7d)), each fabricated with two braiding angles (20° and 40°)—are experimentally evaluated using the Short Beam Shear (SBS) method. In-situ strain fields during testing are recorded by Digital Image Correlation (DIC), and internal damage mechanisms are identified through micro-Computed Tomography (micro-CT). The results indicate that although the shear strength and energy absorption are jointly influenced by both braiding angle and structure, the specimens with a 20° braiding angle generally demonstrate a higher initial modulus, enhanced failure strength, and improved energy absorption relative to those braided at 40°. The damage mechanisms of 3D BCs have significant differences between the four kinds braiding structures, primarily due to the different orientations of the yarns. Furthermore, progressive damage analysis of the 3D BCs specimen reveals that matrix cracking is the initial damage pattern, followed by crack propagation along the braiding yarns and ultimate failure occurs as fiber fracture at the bottom of the specimen.
KW - 3D braided composite
KW - Damage mechanism
KW - Digital image correlation
KW - Micro-computed tomography
KW - Out-of-plane shear performance
UR - https://www.scopus.com/pages/publications/105054870549
U2 - 10.1016/j.cja.2026.104216
DO - 10.1016/j.cja.2026.104216
M3 - 文章
AN - SCOPUS:105054870549
SN - 1000-9361
VL - 39
JO - Chinese Journal of Aeronautics
JF - Chinese Journal of Aeronautics
IS - 12
M1 - 104216
ER -