摘要
Adopting pulsed electro-acoustic method space charge measurement method, space charge profiles and maximal transient fields of polyethylene (PE) films were measured at room temperature (ΔT=0°C) and under temperature gradient (ΔT=40°C), when DC stress of -50 kV/mm was applied for 2 hours and then voltage polarity reverses to stress of 50 kV/mm with the time of 20 s, 30 s and 60 s respectively. The test results show that the faster the voltage reversal at room temperature the higher the maximal transient field. However under temperature gradient (ΔT=40°C), the faster the voltage reversal the lower the maximal transient field, and the time reaching the maximal transient field decreases with the increase of voltage reverse time gradually.
| 源语言 | 英语 |
|---|---|
| 页(从-至) | 105-109 |
| 页数 | 5 |
| 期刊 | Hsi-An Chiao Tung Ta Hsueh/Journal of Xi'an Jiaotong University |
| 卷 | 44 |
| 期 | 10 |
| 出版状态 | 已出版 - 10月 2010 |
学术指纹
探究 'Effect of voltage reverse time on space charge and transient field in polyethylene' 的科研主题。它们共同构成独一无二的指纹。引用此
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver