N2 - [001]-textured 0.4P(Mg1/3Nb2/3)O3-0.25PbZrO3-0.35PbTiO3-0.5%MnO2 (Mn-PMN-PZT) ceramics were fabricated by templated grain growth using 2 vol. % BaTiO3 in this paper. Full matrices of dielectric (ɛij), elastic (sij, cij), and piezoelectric (dij) parameters were obtained by the resonance-antiresonance method. The dielectric constant ɛ33T of textured ceramics reaches 2600, which is four times that of random ceramics. Textured Mn-PMN-PZT ceramics exhibit high d33 = 984 pC/N and high k33 = 0.89, which is much larger than d33 = 223 pC/N and k33 = 0.70 of random ceramics. However, ɛ11T of ceramics decreases by about 30% after texturing, and the corresponding shear coupling coefficient k15 also decreases from 0.66 to 0.44, which may be due to the reduction in the angle between spontaneous polarization and transverse direction. Furthermore, the temperature stability of the textured ceramics was evaluated as well. The phase transition temperature TR−T was determined by the impedance method to be 120 °C. The textured Mn-PMN-PZT ceramic shows high temperature stability, which is better than PMN-PT.
AB - [001]-textured 0.4P(Mg1/3Nb2/3)O3-0.25PbZrO3-0.35PbTiO3-0.5%MnO2 (Mn-PMN-PZT) ceramics were fabricated by templated grain growth using 2 vol. % BaTiO3 in this paper. Full matrices of dielectric (ɛij), elastic (sij, cij), and piezoelectric (dij) parameters were obtained by the resonance-antiresonance method. The dielectric constant ɛ33T of textured ceramics reaches 2600, which is four times that of random ceramics. Textured Mn-PMN-PZT ceramics exhibit high d33 = 984 pC/N and high k33 = 0.89, which is much larger than d33 = 223 pC/N and k33 = 0.70 of random ceramics. However, ɛ11T of ceramics decreases by about 30% after texturing, and the corresponding shear coupling coefficient k15 also decreases from 0.66 to 0.44, which may be due to the reduction in the angle between spontaneous polarization and transverse direction. Furthermore, the temperature stability of the textured ceramics was evaluated as well. The phase transition temperature TR−T was determined by the impedance method to be 120 °C. The textured Mn-PMN-PZT ceramic shows high temperature stability, which is better than PMN-PT.
UR - https://www.scopus.com/pages/publications/85193582432
U2 - 10.1063/5.0212073
DO - 10.1063/5.0212073
M3 - 文章
AN - SCOPUS:85193582432
SN - 0021-8979
VL - 135
JO - Journal of Applied Physics
JF - Journal of Applied Physics
IS - 18
M1 - 184103
ER -