跳到主要导航 跳到搜索 跳到主要内容

Detailed procedures of retrofilling transformers with FR3 natural ester and residual mineral oil content testing

  • Yuan Wang
  • , Ruifeng Wang
  • , Kexin Pan
  • , Yang Xu
  • , Kevin Rapp
  • Xi'an Jiaotong University
  • Shanghai International Commerce Center
  • North China Electric Power University
  • Cargill

科研成果: 期刊稿件文章同行评审

30 引用 (Scopus)

摘要

Several retrofillings have been performed by different utilities in China. However, there is still insufficient understanding of the retrofilling procedures for minimising residual mineral oil and on the effect of the temperature rise of transformers. Following new detailed procedures, an out-of-service S11-M-315/10 (10 kV 315 kVA) and a new S13-M-400/10 (10 kV 400 kVA) distribution transformers were selected to retrofill their mineral oil with FR3, a soybean-based natural ester. A method was proposed to predict the residual mineral oil content, which uses the kinematic viscosity at 60°C. This method fills a gap in the testing of residual mineral oil content. The mass ratios of residual mineral oil were 1.24% for the S11-M-315/10 transformer and 2.05% for the S13-M-400/10 transformer, based on the procedures in this study. The fire point of the mixed oil after retrofilling was 352°C, which meets the K-class less-flammable requirements, indicating a proper control of residual mineral oil. After retrofilling, the time of reaching the limits of the 1.5 times rated load was 30% longer than that of the mineral oil transformer. Two retrofilled transformers have been operating in good conditions since November 2019 for the S11-M-315/10 transformer and December 2020 for the S13-M-400/10 transformer.

源语言英语
页(从-至)1901-1913
页数13
期刊IET Generation, Transmission and Distribution
16
10
DOI
出版状态已出版 - 5月 2022

学术指纹

探究 'Detailed procedures of retrofilling transformers with FR3 natural ester and residual mineral oil content testing' 的科研主题。它们共同构成独一无二的学术指纹。

引用此