N2 - Ultra-high temperature ceramic (UHTC) is one of the most promising materials used in thermal protection system for hypersonic flight vehicles. In this work, ZrB2–0.5 vol% SiC composites are fabricated with nano-sized ZrB2 and SiC particles by spark plasma sintering (SPS) at 1500 °C. The average density of the composites reaches 5.47 g cm−3, while the average grain size is only 1 μm. Then, single and cyclic ablation tests are conducted using a plasma generator. Ablation mechanisms and microstructure evaluation of the composites are discussed in detail. In addition, a digital optical microscope system is adopted to obtain the surface micrograph after ablation. Results show that ablation center will become protuberant rather than form an ablation crater, due to the relative porous and loose oxide layer and flushing action of ablation flame. Thickness of oxide layer and mass gain of the sample obviously increase during the single ablation, while the mass change rate decreases gradually and is then kept stable with the ablation time increasing. Compared with the single ablation, the cyclic ablation leads to higher mass gain and mass change rate, as many microcracks formed on the surface which will significantly accelerate the oxidation.
AB - Ultra-high temperature ceramic (UHTC) is one of the most promising materials used in thermal protection system for hypersonic flight vehicles. In this work, ZrB2–0.5 vol% SiC composites are fabricated with nano-sized ZrB2 and SiC particles by spark plasma sintering (SPS) at 1500 °C. The average density of the composites reaches 5.47 g cm−3, while the average grain size is only 1 μm. Then, single and cyclic ablation tests are conducted using a plasma generator. Ablation mechanisms and microstructure evaluation of the composites are discussed in detail. In addition, a digital optical microscope system is adopted to obtain the surface micrograph after ablation. Results show that ablation center will become protuberant rather than form an ablation crater, due to the relative porous and loose oxide layer and flushing action of ablation flame. Thickness of oxide layer and mass gain of the sample obviously increase during the single ablation, while the mass change rate decreases gradually and is then kept stable with the ablation time increasing. Compared with the single ablation, the cyclic ablation leads to higher mass gain and mass change rate, as many microcracks formed on the surface which will significantly accelerate the oxidation.
KW - ablation test
KW - oxidation reaction
KW - spark plasma sintering
KW - ultra-high temperature ceramic
UR - https://www.scopus.com/pages/publications/85052924819
U2 - 10.1002/adem.201800551
DO - 10.1002/adem.201800551
M3 - 文章
AN - SCOPUS:85052924819
SN - 1438-1656
VL - 20
JO - Advanced Engineering Materials
JF - Advanced Engineering Materials
IS - 11
M1 - 1800551
ER -