Creep life modelling of nickel-based single crystal superalloy DD6 with MCrAlY coating

  • Dongxu Li
  • , Pin Lu
  • , Ziang Li
  • , Wei Zhang
  • , Tao Hua
  • , Xueling Fan
  • Xi'an Jiaotong University
  • AVIC Xi'an Flight Automatic Control Research Institute

科研成果: 期刊稿件文章同行评审

12 引用 (Scopus)

摘要

DD6 single-crystal superalloy is a crucial structural material widely employed in aerospace, energy, and petrochemical industries. High-temperature creep resistance is a critical indicator for evaluating alloys. In this study, a creep lifetime prediction model for DD6 single-crystal alloy was established based on high-temperature creep equations and creep deformation data. By combining theoretical modeling and finite element simulation, a method for predicting the creep behavior of MCrAlY-coated DD6 single crystal alloy was proposed, and the influence of oxide layer thickness and inner wall temperature of thin-walled hollow structures on the second-stage steady-state creep strain rate in the substrate danger zone was investigated. The predictive capability of the model was validated through experiment. The research results indicate that the MCrAlY coating has a minimal impact on the high-temperature creep lifetime of [0 0 1]-oriented DD6 single-crystal superalloy. Pre-exposure treatment thickens the initial oxide layer of the coating, effectively extending the creep lifetime of the coated alloy, particularly at higher temperatures and stress levels. This underscores the effectiveness of pre-exposure treatment in increasing the creep lifetime of the MCrAlY-coated DD6 single-crystal superalloy system. The influence of inner wall temperature in thin-walled hollow structures on creep lifetime follows a parabolic pattern. Excessively low inner wall temperatures reduce creep lifetime due to significant thermal mismatch stresses, while excessively high inner wall temperatures decrease creep lifetime because of changes in material properties at those temperatures. The proposed model provide valuable insights into the creep lifetime prediction of [0 0 1]-oriented DD6 single-crystal superalloy with an MCrAlY coating.

源语言英语
文章编号110194
期刊Engineering Fracture Mechanics
306
DOI
出版状态已出版 - 5 8月 2024

学术指纹

探究 'Creep life modelling of nickel-based single crystal superalloy DD6 with MCrAlY coating' 的科研主题。它们共同构成独一无二的指纹。

引用此