摘要

After the Fukushima explosion, the research and development of accident tolerant fuel (ATF) cladding has become a hot spot in the nuclear field. In this work, corrosion behavior of Zircaloy-4, Zr-1Nb and FeCrAl alloys was investigated in deaerated water at 330 °C and 14 MPa. All alloys were found to lose weight. In Li/B water, the corrosion resistance followed an order of FeCrAl > Zr-1Nb > Zircaloy-4. Local corrosion occurred on the Zircaloy-4 surface and developed towards the interior of the matrix, leading to selective oxidation. A certain thickness of oxide layer was formed on the surface of Zr-1Nb, but the distribution was uneven. Significant oxide exfoliation made Zr-1Nb display complex defects. The oxide film of FeCrAl alloy had a double-spinel structure. Low surface adsorption energy and weak interaction between Fe and O atoms is responsible for superior corrosion resistance of FeCrAl alloy.

源语言英语
文章编号142143
期刊Chemical Engineering Journal
462
DOI
出版状态已出版 - 15 4月 2023

学术指纹

探究 'Corrosion of Zircaloy-4, Zr-1Nb and FeCrAl alloys in deaerated water at 330 °C and 14 MPa: Superior corrosion resistance and corrosion mechanism of FeCrAl alloy by experiments and molecular dynamics simulations' 的科研主题。它们共同构成独一无二的指纹。

引用此