TY - JOUR
T1 - CoMoCrSi coatings prepared by high-velocity oxygen fuel spraying
T2 - Microstructure and mechanical properties at elevated temperatures up to 800 °c
AU - Guo, Hongjian
AU - Wang, Yijing
AU - Hao, Enkang
AU - Li, Bo
AU - An, Yulong
AU - Chen, Jianmin
AU - Zhou, Huidi
AU - Yan, Pengxun
AU - Wu, Zhiguo
N1 - Publisher Copyright:
© 2020 IOP Publishing Ltd.
PY - 2019
Y1 - 2019
N2 - The microstructures, mechanical properties, and tribological behaviors from room temperature (RT) to 800 °C of HOVF-sprayed CoMoCrSi coatings were investigated in detail. The as-sprayed CoMoCrSi coatings were found to be predominantly composed of intermetallic Laves phases, i.e., Co7Mo6, Co3Mo2Si, Cr3Si, and some amorphous phases. The as-sprayed coatings possessed a compact and typical lamellar microstructure and balanced mechanical property; their Vickers hardness decreased from 855.9 ± 16 HV5.0 at RT to 583.9 ± 10 HV5.0 at 800 °C due to a normal soft phenomenon of material in hot environment. Further, between room temperature and 400 °C, the as-sprayed coatings suffered serious mechanical wear without any lubricant tribolayer forming on the worn surface, indicating that they would not function as good anti-wear materials at low temperatures. In particular, the coatings exhibited a brittle fracture coupled with abrasive wear at RT, obvious abrasive wear at 200 °C, and severe adhesive wear at 400 °C that with the highest friction coefficient of 0.65 and wear rate of 35.79 × 10-6mm3/(N•m). As the test temperature increased to 600 and 800 °C, the friction coefficient of the coating decreased to 0.45 and 0.26, respectively, and the corresponding wear rates reached 0.135 × 10-6mm3/(N•m) and 0.288 × 10-6 mm3/(N•m), with a difference of approximately two orders of magnitude between the low- and high-temperature wear rate. This result further confirmed that the as-sprayed coatings are a better choice of abrasion-resistant materials for high-temperature applications. After sliding tests at 800 °C, numerous metallic oxides i.e., Co3O4, MoO3, and bimetallic oxides such as CoMoO4 and Co2CrO4 of nanometer size (50-100 nm) were identified in the continuous protective layer formed on the worn surface. These oxides played an important role of lubrication and reduced direct contact between the coating and its counterpart during the sliding process, leading to a decrease in the friction coefficient and material loss. The main wear mechanisms of the coatings at this temperature range are slight adhesive wear coupled with abrasive wear.
AB - The microstructures, mechanical properties, and tribological behaviors from room temperature (RT) to 800 °C of HOVF-sprayed CoMoCrSi coatings were investigated in detail. The as-sprayed CoMoCrSi coatings were found to be predominantly composed of intermetallic Laves phases, i.e., Co7Mo6, Co3Mo2Si, Cr3Si, and some amorphous phases. The as-sprayed coatings possessed a compact and typical lamellar microstructure and balanced mechanical property; their Vickers hardness decreased from 855.9 ± 16 HV5.0 at RT to 583.9 ± 10 HV5.0 at 800 °C due to a normal soft phenomenon of material in hot environment. Further, between room temperature and 400 °C, the as-sprayed coatings suffered serious mechanical wear without any lubricant tribolayer forming on the worn surface, indicating that they would not function as good anti-wear materials at low temperatures. In particular, the coatings exhibited a brittle fracture coupled with abrasive wear at RT, obvious abrasive wear at 200 °C, and severe adhesive wear at 400 °C that with the highest friction coefficient of 0.65 and wear rate of 35.79 × 10-6mm3/(N•m). As the test temperature increased to 600 and 800 °C, the friction coefficient of the coating decreased to 0.45 and 0.26, respectively, and the corresponding wear rates reached 0.135 × 10-6mm3/(N•m) and 0.288 × 10-6 mm3/(N•m), with a difference of approximately two orders of magnitude between the low- and high-temperature wear rate. This result further confirmed that the as-sprayed coatings are a better choice of abrasion-resistant materials for high-temperature applications. After sliding tests at 800 °C, numerous metallic oxides i.e., Co3O4, MoO3, and bimetallic oxides such as CoMoO4 and Co2CrO4 of nanometer size (50-100 nm) were identified in the continuous protective layer formed on the worn surface. These oxides played an important role of lubrication and reduced direct contact between the coating and its counterpart during the sliding process, leading to a decrease in the friction coefficient and material loss. The main wear mechanisms of the coatings at this temperature range are slight adhesive wear coupled with abrasive wear.
KW - CoMoCrSi coating
KW - high-velocity oxygen fuel spraying
KW - microstructure
KW - tribological performance
KW - wear mechanism
UR - https://www.scopus.com/pages/publications/85081789254
U2 - 10.1088/2053-1591/ab6374
DO - 10.1088/2053-1591/ab6374
M3 - 文章
AN - SCOPUS:85081789254
SN - 2053-1591
VL - 6
JO - Materials Research Express
JF - Materials Research Express
IS - 12
M1 - 1265E9
ER -