TY - JOUR
T1 - Achieving fully-equiaxed fine β-grains in laser-additive-manufactured Sn-free high-temperature titanium alloy designed by cluster formula
AU - Zhu, Zhihao
AU - Wang, Jian
AU - Lü, Zhidan
AU - Niu, Jingzhe
AU - Zhang, Xuezhe
AU - Liu, Nan
AU - Jia, Liang
AU - Zhang, Jinyu
N1 - Publisher Copyright:
© 2025 The Authors
PY - 2025/3/1
Y1 - 2025/3/1
N2 - Conventional high-temperature titanium alloys contain Sn as their essential alloying element. Upon additive manufacturing, these alloys exhibit insufficient mechanical properties due to the presence of coarse β-columnar grains. In this work, Sn-free high-temperature Ti-5.5Al-11.2Zr-4.8Ta-1.6W-0.5Si alloy with fully-equiaxed fine β grains was designed targeted for additive manufacturing on the basis of the composition formula of Ti65 alloy. This alloy shows good additive manufacturability and tensile strengths. Its composition formula satisfy α-{[Al–Ti12](AlTi2)}12+β-{[(Al–Ti10.5Zr3.5](Ta0.75W0.25Ti1.5Si0.5)}5, featuring equiaxed β grains via Ta replacing Mo/Nb and enhanced additive-manufacturability via Zr replacing Sn. In the as-deposited state, this alloy shows complete equiaxed fine β grains and inner with bimodal basket-weave microstructure, as well as excellent tensile properties (ultimate tensile strength (UTS) of 1312 MPa, yield strength (YS) of 1258 MPa, and elongation of 1.8%). Its 600 °C UTS of 703 MPa, YS of 551 MPa, and elongation of 18%, being comparable to those wrought conventional high-temperature Ti alloys.
AB - Conventional high-temperature titanium alloys contain Sn as their essential alloying element. Upon additive manufacturing, these alloys exhibit insufficient mechanical properties due to the presence of coarse β-columnar grains. In this work, Sn-free high-temperature Ti-5.5Al-11.2Zr-4.8Ta-1.6W-0.5Si alloy with fully-equiaxed fine β grains was designed targeted for additive manufacturing on the basis of the composition formula of Ti65 alloy. This alloy shows good additive manufacturability and tensile strengths. Its composition formula satisfy α-{[Al–Ti12](AlTi2)}12+β-{[(Al–Ti10.5Zr3.5](Ta0.75W0.25Ti1.5Si0.5)}5, featuring equiaxed β grains via Ta replacing Mo/Nb and enhanced additive-manufacturability via Zr replacing Sn. In the as-deposited state, this alloy shows complete equiaxed fine β grains and inner with bimodal basket-weave microstructure, as well as excellent tensile properties (ultimate tensile strength (UTS) of 1312 MPa, yield strength (YS) of 1258 MPa, and elongation of 1.8%). Its 600 °C UTS of 703 MPa, YS of 551 MPa, and elongation of 18%, being comparable to those wrought conventional high-temperature Ti alloys.
KW - Cluster formula
KW - Laser additive manufacturing
KW - Mechanical properties
KW - Ti alloys
UR - https://www.scopus.com/pages/publications/85219497327
U2 - 10.1016/j.jmrt.2025.03.017
DO - 10.1016/j.jmrt.2025.03.017
M3 - 文章
AN - SCOPUS:85219497327
SN - 2238-7854
VL - 35
SP - 6408
EP - 6420
JO - Journal of Materials Research and Technology
JF - Journal of Materials Research and Technology
ER -