跳到主要导航 跳到搜索 跳到主要内容

锌灰资源化回收及超临界水热合成 纳米氧化锌系统工艺

  • Lu Liu
  • , Shuzhong Wang
  • , Wei Liu
  • , Baoquan Zhang
  • , Hui Liu
  • , Jun'An Zhao
  • Xi'an Jiaotong University

科研成果: 期刊稿件 › 文章 › 同行评审

摘要

In this study, a combination of wet recovery process and supercritical hydrothermal synthesis technology is employed to produce high-value nano-zinc oxide products from zinc ash? and an economic analysis of this approach to zinc ash recycling is conducted. A sound system is established using Aspen Plus, and material costs and energy consumption during system operation are analyzed. The leaching rate of zinc in the zinc ash exceeds 95%, under the conditions of sulfuric acid concentration of 2 mol • L-1, solid-liquid ratio of 1:8, leaching temperature of 50 °C, leaching time of 2 h, and stirrer speed of 300 r • min-1. Fe, Al, Ni, Cu and other impurities are eliminated in the impurity removal process, and the zinc content in the solution after impurity removal reaches 97%. The leaching solution of zinc ash is used to synthesize nano-zinc oxide with an average particle size of 26 nm under supercritical conditions of 400 °C and 25 MPa. The resulting zinc oxide exhibits excellent crystallinity and high purity. The comparison with nano-zinc oxide synthesized from pure materials validates the feasibility of this technology, which significantly improves the system?s economic viability.

投稿的翻译标题Zinc Ash Recycling and the System of Supercritical Hydrothermal Synthesis of Nano-Zinc Oxide
源语言繁体中文
页(从-至)193-203
页数11
期刊Hsi-An Chiao Tung Ta Hsueh/Journal of Xi'an Jiaotong University
卷58
期3
DOI
出版状态已出版 - 3月 2024

联合国可持续发展目标

此成果有助于实现下列可持续发展目标:

  1. 可持续发展目标 7 - 经济适用的清洁能源
    可持续发展目标 7 经济适用的清洁能源

关键词

  • high-value utilization
  • nano-zinc oxide
  • recycling of zinc ash
  • supercritical hydrothermal synthesis

学术指纹

探究 '锌灰资源化回收及超临界水热合成 纳米氧化锌系统工艺' 的科研主题。它们共同构成独一无二的学术指纹。

引用此