The high-purity tantalum after cold deformation was annealed at different temperatures (850-1050 °C). The regularity of microstructure and texture evolution, the dependence of recrystallized nucleation and orientation, and the effect of recrystallized structure on its mechanical behavior were studied after annealing. The results show that the cold-deformed microstructure is the fibrous structure with {100} and {111} orientations, which is dominated by the α-fibre of (001)[110 ] component. After annealing, the microstructure of high-purity tantalum is in the recovery stage (850 °C), complete recrystallization (950 °C) and grain growth stage (1050 °C). With the increase in annealing temperature, the α-fibre gradually weakens and then the γ-fibre gradually forms, especially the α-fibre disappears completely after recrystallization. The yield strength and strain hardening ability decrease with the increase in annealing temperature, and the plasticity is significantly improved, especially the uniform elongation reaches 17.85% after recrystallization. When the annealing temperature is increased to 1050 °C, the intergranular fracture of the secondary recrystallized grains is prone to occur, resulting in poor mechanical properties.

投稿的翻译标题Effect of Annealing Temperature on Recrystallization Texture and Mechanical Behavior of High Purity Tantalum Used for Tantalum Fiber
源语言繁体中文
页(从-至)2869-2875
页数7
期刊Xiyou Jinshu Cailiao Yu Gongcheng/Rare Metal Materials and Engineering
卷52
期8
出版状态已出版 - 8月 2023

关键词

  • annealing temperature
  • high-purity tantalum
  • mechanical properties
  • recrystallized texture
  • strain hardening behavior