Hindered phenol AO-60/nitrile butadiene rubber-epoxidized natural rubber-natural rubber composites were prepared by using hindered phenol AO-60/nitrile butadiene rubber (NBR) (mass ratio 40:100) as damping phase and epoxidized natural rubber (ENR) as compatibilizer. It is found that the microstructure of the composites is "sea-island structure" and the co-continuous morphology appears when the mass ratio of NR/NBR is 60:40 and 50:50. The composite exhibit two glass transition temperatures, which occur near -60℃ and around -10℃. With the increase of mass ratio of AO-60/NBR, the effective damping of the composite in the temperature range of -20-40℃ is widened from 0℃ to 35.9℃, and the loss factor increases slightly with increasing strain. The composites exhibit low stress at low strain and exhibits high flexibility. At the same time, it has a stress crack point at higher strain, showing high tensile strength and elongation at break.
| 投稿的翻译标题 | Preparation and damping properties of hindered phenol AO-60/nitrile butadiene rubber-epoxidized natural rubber-natural rubber composites |
|---|---|
| 源语言 | 繁体中文 |
| 页(从-至) | 1796-1803 |
| 页数 | 8 |
| 期刊 | Fuhe Cailiao Xuebao/Acta Materiae Compositae Sinica |
| 卷 | 36 |
| 期 | 8 |
| DOI | |
| 出版状态 | 已出版 - 1 8月 2019 |
| 已对外发布 | 是 |
关键词
- Compatibilizer
- Composites
- Damping properties
- Isolation bearing
- Rubber
学术指纹
探究 '受阻酚AO-60/丁腈橡胶-环氧化天然橡胶-天然橡胶复合材料的制备及其阻尼性能' 的科研主题。它们共同构成独一无二的指纹。引用此
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver