Abstract
Harnessing the full potential of Ni-rich single-crystal cathodes (LiNixMnyCo1-x-yO2, NMC) for next-generation high-energy lithium batteries is hindered by their slow reaction kinetics and susceptibility to interfacial decay. Our research introduces a novel strategy utilizing triethyl phosphate (TEP) and fluoroethylene carbonate (FEC) to optimize the Li+ solvation environment, lowering the coordination number and diminishing the energy threshold for Li+ transport. Mechanistic studies indicate that this intervention not only accelerates the Li+ transfer at the electrode/electrolyte interface but also catalyzes the development of a robust LiF-rich CEI layer. As a result, the single-crystal NMC83 cathode exhibits remarkable high-rate discharge capacities of approximately 209 mAh g−1 at 0.1 C and 192 mAh g−1 at 0.5 C. The robust CEI layer also mitigates parasitic reactions, substantially improving the cycle life, with capacity retention increasing from 46.1 % to 88.2 % after 300 cycles at 1 C. This work underscores the transformative impact of solvation sheath engineering on the interfacial dynamics of single-crystal cathodes, paving the way for more durable and efficient energy storage solutions.
| Original language | English |
|---|---|
| Article number | 110276 |
| Journal | Nano Energy |
| Volume | 131 |
| DOIs | |
| State | Published - 1 Dec 2024 |
| Externally published | Yes |
UN SDGs
This output contributes to the following UN Sustainable Development Goals (SDGs)
-
SDG 7 Affordable and Clean Energy
Keywords
- Cathode-electrolyte interphase
- Fast interfacial kinetics
- Flame-retardant
- Single crystal Ni-rich cathode
- Solvation sheath