Skip to main navigation Skip to search Skip to main content

Temperature-triggered wetting transition and interfacial activation of Ti/TiN-modified ZTA ceramics by molten high-chromium cast iron

  • Yefei Li
  • , Yanmei Yang
  • , Fangyu Zhu
  • , Zihan Wu
  • , Zilong Zhao
  • , Yong Wang
  • Xinjiang University
  • Xi'an Jiaotong University
  • Ltd.
  • The12th Research Institute of China Shipbuilding Group Corporation

Research output: Contribution to journal › Article › peer-review

Abstract

Poor wettability between oxide ceramics and iron-based melts remains a critical obstacle to the fabrication of reliable ceramic-reinforced iron-matrix composites. In this work, Ti and TiN interlayers were introduced onto zirconia-toughened alumina (ZTA) ceramics to regulate the wetting behavior and interfacial reactions with high-chromium cast iron (HCCI). The Ti-coated ZTA exhibited a temperature-triggered wetting transition: the final contact angle remained approximately 70° at 1420 °C because an Al/O-rich interfacial layer partially hindered direct interaction between the molten alloy and the Ti coating, whereas it sharply decreased to approximately 15° at 1440 °C and further to approximately 11° at 1460 °C after disruption of this barrier. In contrast, the TiN-modified interface showed delayed wetting activation due to the higher chemical stability of TiN, but achieved a similar final contact angle of approximately 11° at 1460 °C while maintaining a relatively continuous interfacial layer. Microstructural and elemental analyses suggested that active Ti-containing species were associated with local elemental redistribution, including Zr/Al/O redistribution and reaction-assisted penetration of Fe and Cr into the ceramic side. Spreading kinetic analysis further indicated that the initial rapid spreading was mainly associated with adsorption and migration of active Ti species, whereas the later stage was governed by diffusion-assisted interfacial reactions. These results demonstrate two distinct but convergent wetting activation routes for designing stable ZTA/high-chromium cast iron interfaces.

Original languageEnglish
JournalCeramics International
DOIs
StateAccepted/In press - 2026

Keywords

  • High-chromium cast iron
  • Interfacial reaction
  • Ti interlayer
  • TiN interlayer
  • Wetting
  • ZTA ceramic

Fingerprint

Dive into the research topics of 'Temperature-triggered wetting transition and interfacial activation of Ti/TiN-modified ZTA ceramics by molten high-chromium cast iron'. Together they form a unique fingerprint.

Cite this