Regeneration of sulfur poisoning Cu-Ir/H-ZSM-5catalyst in catalytic reduction of NOx with propane by H2 reduction

  • Hua Pan
  • , Yan Fei Jian
  • , Yu Hui Guo
  • , Ning Na Chen
  • , Chi He
  • Xi'an Jiaotong University
  • CAS - Institute of Earth Environment

Research output: Contribution to journalArticlepeer-review

Abstract

Effect of regeneration parameters of H2 reduction on sulfur poisoning Cu-Ir/H-ZSM-5catalyst for catalytic reduction of NOx with propane (C3H8-SCR) was investigated. The regeneration behavior was carried out by N2 adsorption, X-ray diffraction (XRD), X-ray photoelectron spectrometer (XPS) and hydrogen temperature-programmed reduction (H2-TPR). Deactivation of Cu-Ir/H-ZSM-5was caused by the formation of CuSO4, resulting in the loss of the active sites, decrease of the surface area, microspore area and pore volume of catalyst. The temperature of 500℃ and regeneration gas consumption of 42.8 L/gcatalyst were the best regeneration condition for H2 reduction, because of the lowest content (0.4%) of CuSO4 on Cu-Ir/H-ZSM-5catalyst. The activity of Cu-Ir/H-ZSM-5catalyst regenerated could be returned to 95% of the fresh catalyst. The increase of the surface area, microspore area, and pore volume of catalyst was obtained by H2 reduction.

Original languageEnglish
Pages (from-to)1360-1365
Number of pages6
JournalZhongguo Huanjing Kexue/China Environmental Science
Volume36
Issue number5
StatePublished - 1 May 2016

Keywords

  • Catalytic reduction by CH
  • Cu-Ir/H-ZSM-5catalyst
  • H reduction regeneration
  • Sulfur poisoning