Skip to main navigation Skip to search Skip to main content

RB-SiC ceramics derived from the phenol resin added with starch

  • Xi'an Jiaotong University

Research output: Contribution to journal › Article › peer-review

4 Scopus citations

Abstract

Reaction bonded silicon carbide (RB-SiC) was fabricated by phenol resin, starch, solidified agent and silicon powder through the following steps: first, carbonizing at high temperature for 7-9h, infiltrating silicon at 1450-1600°C for 0.5-2H, and then removing excessive silicon at 1700°C for 0.5h. Scanning electron microscopy and X-ray diffraction were employed to characterize and analyze the microstructures and phase composition of the preforms and the final RB-SiC products. In addition, the effect of carbonization temperature, the amount of starch and solidified agent on strength and apparent porosity of final RB-SiC were also discussed. The results showed that the carbonization process of phenol resin can be divided into three steps: at temperatures from 400°C to 600°C, the structure of polymer changes less; at temperatures from 600°C to 1000°C, the fundamental chain of polymer is destroyed, and inverts to glass-like carbon; at temperatures from 1000°C to 1200°C, with the increasing of carbonization temperature, the structure of glass-like carbon changes into the structure of disorder graphite. And the increased micro-pores could be obtained by adding starch.

Original languageEnglish
Pages (from-to)1144-1147
Number of pages4
JournalKey Engineering Materials
Volume336-338 II
DOIs
StatePublished - 2007

Keywords

  • Phenol resin
  • Reaction bonded
  • Silicon carbide

Fingerprint

Dive into the research topics of 'RB-SiC ceramics derived from the phenol resin added with starch'. Together they form a unique fingerprint.

Cite this