Abstract
xLi2Mn03·(l-x)LiNi1/3Co1/3Mn1/3O2 (x=0.1, 0.2, 0.3 and 0.4) solid solutions were prepared by annealing the precursors at 900 °C for 12 h, which were dried from the mixtures of LiNi1/3Co1/3Mn1/3O2 powder and the solutions of LiNO3 and Mn (NO3)2. The peaks intensity of solid solutions XRD patterns were weak and broaden. The structure peaks (LiMn6) in 20° ~30° became more clearly with the x value. The size of single particles increased from 250 nm of x =0.1 to 350 nm of x =0.4 although the appearance of these solid solutions were agglomerate. The capacities of the solid solutions increased with the voltage increasing. The electrode polarization was least and the discharge plateau was highest at x=0.2 from the charge and discharge curves within 2.5~4.6 V. Furthermore, the capacity retention ratios increased from 91.2% to 105.6% with x value after different rate cycling 21 cycles. The results showed that the electrochemical properties of LiNi1/3Co1/3Mn1/3O2 materials can be improved by Li2MnO3.
| Original language | English |
|---|---|
| Pages (from-to) | 1125-1130 |
| Number of pages | 6 |
| Journal | Chinese Journal of Inorganic Chemistry |
| Volume | 28 |
| Issue number | 6 |
| State | Published - Jun 2012 |
UN SDGs
This output contributes to the following UN Sustainable Development Goals (SDGs)
-
SDG 7 Affordable and Clean Energy
Keywords
- Cathode material
- Lithium ion battery
- Solid solution
Fingerprint
Dive into the research topics of 'Properties study of xLi2MnO3 · (l-x) LiNi1/3 Mn1/3O2 (x=0.1, 0.2, 0.3 and 0.4) solid solution materials'. Together they form a unique fingerprint.Cite this