Abstract
Nanocrystalline Ti(CxN1 - x) films on titanium were prepared by plasma electrolytic carbonitriding (PEC/N) at 600 V in an electrolytic solution containing triethanolamine and formamide using a pulse power supply. XRD, EDAX, FESEM and TEM were employed to characterize the phase components, element composition, and microstructure of the films. Rockwell C indenter and Vicker's indentation test were used to evaluate the adhesion and hardness of the films. The obtained results show that the films are porous and composed of Ti(CxN1 - x), without apparent discontinuity in the interfaces adjacent to the titanium substrate. The thickness, ratios of C/N and pores sizes of the films tend to increase with the discharge time. When discharge-treated for 2.5 h, the film is about 15 μm thick and exhibits nanocrystalline characterization with grain size of 40-60 nm. Its hardness is Hv 2083 at the load of 0.2 N and the adhesion, Pc value, is more than 500 N. The formation process and mechanism of the Ti(CxN1 - x) films are discussed.
| Original language | English |
|---|---|
| Pages (from-to) | 267-272 |
| Number of pages | 6 |
| Journal | Electrochemistry Communications |
| Volume | 8 |
| Issue number | 2 |
| DOIs | |
| State | Published - Feb 2006 |
Keywords
- Nanocrystalline
- Plasma electrolytic carbonitriding
- Ti(CN) thick film
Fingerprint
Dive into the research topics of 'Porous nanocrystalline Ti(CxN1 - X) thick films by plasma electrolytic carbonitriding'. Together they form a unique fingerprint.Cite this
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver