TY - GEN
T1 - Non-debye dielectric behavior of aged XLPE cable insulation
AU - Zhang, Yuanyuan
AU - Wu, Kangning
AU - Zhao, Chun
AU - Xiang, Jiao
AU - Li, Jianying
AU - Li, Shengtao
N1 - Publisher Copyright:
© 2018 IEEE.
PY - 2018/6/29
Y1 - 2018/6/29
N2 - In this study, dielectric responses of aged XLPE cable insulation were investigated. Thermal aging experiment was performed on XLPE sheets cut from 110 kV power cable insulation under 130 oC for 10, 20, and 50 days, respectively. The dielectric spectra of all the samples were measured at different temperatures in a frequency range from 10-1 to 106 Hz. An improved analytical methodology, the derivation of real permittivity respect to natural logarithm of angular frequency (∂/∂lnω) was applied in this paper. From experimental results, a new dielectric loss peak appeared in the aged XLPE samples. This new peak showed non-Debye dielectric behavior since it shifted to lower frequency as test temperature increased. Besides, the ∂/∂lnω spectroscopy of four samples showed a clear loss peak moving to lower frequency and becoming more intense with increasing aging time while dielectric loss spectroscopy presented blurry information. The non-Debye dielectric behavior of XLPE samples might be related to the movement of large molecular chains under higher temperature. However, further research is required to understand this behavior completely.
AB - In this study, dielectric responses of aged XLPE cable insulation were investigated. Thermal aging experiment was performed on XLPE sheets cut from 110 kV power cable insulation under 130 oC for 10, 20, and 50 days, respectively. The dielectric spectra of all the samples were measured at different temperatures in a frequency range from 10-1 to 106 Hz. An improved analytical methodology, the derivation of real permittivity respect to natural logarithm of angular frequency (∂/∂lnω) was applied in this paper. From experimental results, a new dielectric loss peak appeared in the aged XLPE samples. This new peak showed non-Debye dielectric behavior since it shifted to lower frequency as test temperature increased. Besides, the ∂/∂lnω spectroscopy of four samples showed a clear loss peak moving to lower frequency and becoming more intense with increasing aging time while dielectric loss spectroscopy presented blurry information. The non-Debye dielectric behavior of XLPE samples might be related to the movement of large molecular chains under higher temperature. However, further research is required to understand this behavior completely.
UR - https://www.scopus.com/pages/publications/85049832028
U2 - 10.1109/ICPADM.2018.8401040
DO - 10.1109/ICPADM.2018.8401040
M3 - 会议稿件
AN - SCOPUS:85049832028
T3 - Proceedings of the IEEE International Conference on Properties and Applications of Dielectric Materials
SP - 435
EP - 438
BT - ICPADM 2018 - 12th International Conference on the Properties and Applications of Dielectric Materials
PB - Institute of Electrical and Electronics Engineers Inc.
T2 - 12th International Conference on the Properties and Applications of Dielectric Materials, ICPADM 2018
Y2 - 20 May 2018 through 24 May 2018
ER -