Abstract
The size-dependent hardness, strain-rate sensitivity (SRS) and shear transformation zone (STZ) volume of co-sputtered Cu–Zr metallic glass films with film thickness h spanning from 1000 to 3000 nm were systematically investigated by nanoindentation creep tests at room temperature. Experimental results manifested an exceptional decrease in hardness and a monotonic increment in SRS (or a monotonic decline in STZ volume) with reducing h. The deformation mechanism could be rationalized in light of more free volume combined with smaller STZs in thinner films, which likely trigger the strain-softening behavior. Moreover, STZs and deformation-induced devitrification promote the homogeneous-like plastic flow. IMPACT STATEMENT Employing nanoindentation creep tests revealed size-dependent hardness and strain-rate sensitivity in metallic glass films, enabling comprehensive understanding of the deformation mechanism based on atomic-scale shear transformation zone theory.
| Original language | English |
|---|---|
| Pages (from-to) | 22-28 |
| Number of pages | 7 |
| Journal | Materials Research Letters |
| Volume | 6 |
| Issue number | 1 |
| DOIs | |
| State | Published - 2 Jan 2018 |
Keywords
- Metallic glass films
- hardness
- nanoindentation
- strain-rate sensitivity
Fingerprint
Dive into the research topics of 'Nanoindentation creep behavior of Cu–Zr metallic glass films'. Together they form a unique fingerprint.Cite this
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver