TY - JOUR
T1 - Multifunctional Vitrimer-Like Polydimethylsiloxane (PDMS)
T2 - Recyclable, Self-Healable, and Water-Driven Malleable Covalent Networks Based on Dynamic Imine Bond
AU - Feng, Zhanbin
AU - Yu, Bing
AU - Hu, Jing
AU - Zuo, Hongli
AU - Li, Jianping
AU - Sun, Haibin
AU - Ning, Nanying
AU - Tian, Ming
AU - Zhang, Liqun
N1 - Publisher Copyright:
© 2019 American Chemical Society.
PY - 2019/1/23
Y1 - 2019/1/23
N2 - Vitrimer is a new class of polymeric materials which can be reprocessed to any shape while being permanently cross-linked. We designed and synthesized a catalyst-free network with poly(dimethylsiloxane)etherimide (PDMS-NH 2 ), terephthalaldehyde (TA), and tri(2-aminoethyl)amine (TREA) through the condensation reaction between amino groups and aldehyde groups. As a result of the exchange reaction of the dynamic imine bond obtained, this PDMS network exhibits the nature of vitrimer-like material, which is examined by solubility and stress-relaxation experiments, and the relaxation time is as short as 64 s at 130 °C. In addition, the vitrimer-like PDMS is malleable and capable of self-healing, and the mechanical properties can be maintained even after three consecutive breaking/mold pressing cycles. Especially, besides heating, this vitrimer-like PDMS can also be recycled and reshaped at ambient temperature due to the exchange reaction of dynamic imine bond when immersed in water, which will potentially lead to green processing of the elastomers.
AB - Vitrimer is a new class of polymeric materials which can be reprocessed to any shape while being permanently cross-linked. We designed and synthesized a catalyst-free network with poly(dimethylsiloxane)etherimide (PDMS-NH 2 ), terephthalaldehyde (TA), and tri(2-aminoethyl)amine (TREA) through the condensation reaction between amino groups and aldehyde groups. As a result of the exchange reaction of the dynamic imine bond obtained, this PDMS network exhibits the nature of vitrimer-like material, which is examined by solubility and stress-relaxation experiments, and the relaxation time is as short as 64 s at 130 °C. In addition, the vitrimer-like PDMS is malleable and capable of self-healing, and the mechanical properties can be maintained even after three consecutive breaking/mold pressing cycles. Especially, besides heating, this vitrimer-like PDMS can also be recycled and reshaped at ambient temperature due to the exchange reaction of dynamic imine bond when immersed in water, which will potentially lead to green processing of the elastomers.
UR - https://www.scopus.com/pages/publications/85060011338
U2 - 10.1021/acs.iecr.8b05309
DO - 10.1021/acs.iecr.8b05309
M3 - 文章
AN - SCOPUS:85060011338
SN - 0888-5885
VL - 58
SP - 1212
EP - 1221
JO - Industrial and Engineering Chemistry Research
JF - Industrial and Engineering Chemistry Research
IS - 3
ER -