The Ti2AlNb alloys suffer from intrinsic brittleness, which creates a persistent trade-off between strength and ductility at room temperature, and also exhibit insufficient high-temperature strength. To address these limitations, we designed a Ti-22Al-25Nb-1Mo-1Zr-0.25Si (at.%) alloy with a controlled near-equiaxed microstructure consisting of the B2 matrix and O precipitates. The B2/O interface with a lattice mismatch of ∼0.021 facilitates dislocation slip transfer and delays crack initiation. The multi-element co-addition of Mo, Zr and Si refines the grain size, reduces the hardness mismatch between the two phases, and provides sustained solid-solution strengthening. These synergistic effects enable the alloy to achieve a yield strength of approximately 1273 MPa and a fracture elongation of about 11.8% at room temperature, substantially outperforming conventional Ti2AlNb alloys. Remarkably, at 650 °C and 750 °C, the designed alloy retains high yield strengths of about 940 and 732 MPa, with ultimate tensile strengths of about 986 and 873 MPa, respectively. Our findings offer a pathway to overcome the strength-ductility paradox in Ti2AlNb alloys through grain boundary engineering and microstructural control.
| Original language | English |
|---|---|
| Article number | 122884 |
| Journal | Acta Materialia |
| Volume | 322 |
| DOIs | |
| State | Published - 1 Jan 2027 |
Keywords
- Deformation mechanisms
- Interfaces
- Mechanical properties
- TiAlNb
Fingerprint
Dive into the research topics of 'Multi-element co-addition achieves ultrahigh strength in a ductile Ti2AlNb alloy from room temperature to 750 °C'. Together they form a unique fingerprint.Cite this
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver