Abstract
In this study, Zr-2.5 Nb alloy was examined after annealing at 560 ℃ under four prior processing conditions: without hot rolling and after hot rolling at 620, 710, and 850 ℃. EBSD and TEM were used to investigate how these conditions affected the final microstructure and mechanical properties. All annealed specimens consisted mainly of α-Zr, with only approximately 0.1% β-Zr detected by EBSD. The UNHR + HT specimen had an average grain size of 0.48 μm. For the HR + HT specimens, the average grain size increased from 0.69 μm at 620 ℃ to 0.78 μm at 710 ℃ and then decreased to 0.67 μm at 850 ℃. The specimen hot rolled at 620 ℃ and subsequently annealed exhibited the most uniform grain structure. In contrast, the 850 ℃ HR + HT specimen showed a necklace structure consisting of lamellar grains and numerous fine grains along the grain boundaries. This feature is related to the greater contribution of DDRX during prior hot rolling at 850 ℃, whereas the microstructures of the 620 and 710 ℃ HR + HT specimens mainly retained features associated with CDRX during hot rolling. TEM observations revealed regions with low dislocation density and limited lattice distortion in the annealed specimens. Nanoscale FCC-related twin features were still observed in the 620 ℃ HR + HT specimen. This specimen exhibited enhanced strength and considerable ductility, achieving an ultimate tensile strength of 593 MPa and an elongation of 38.9%.
| Original language | English |
|---|---|
| Article number | 191757 |
| Journal | Journal of Alloys and Compounds |
| Volume | 1083 |
| DOIs | |
| State | Published - 5 Nov 2026 |
Keywords
- Annealing
- Hot rolling
- Recrystallization
- Ultimate tensile strength
- Zr-2.5 Nb alloy
Fingerprint
Dive into the research topics of 'Microstructure and mechanical properties of Zr-2.5 Nb alloy hot-rolled at different temperatures and subsequently annealed'. Together they form a unique fingerprint.Cite this
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver