Skip to main navigation Skip to search Skip to main content

Microstructural evolution and simultaneous strengthening and toughening of core-shell Mg3Bi2 reinforced Zn-1.2 wt% Mg zinc alloys

  • Ping Lv
  • , Yusheng Liu
  • , Shengqiang Ma
  • , Yang Luo
  • , Yimin Gao
  • , Jiankang Zhang
  • , Jiandong Xing
  • Xi'an Jiaotong University
  • Shaanxi Union Research Center of University and Enterprise for Zinc-Based New Materials

Research output: Contribution to journalArticlepeer-review

Abstract

Microstructure evolution and simultaneous strengthening and toughening of core-shell Mg3Bi2 reinforced Zn-1.2 wt% Mg zinc alloys were investigated. The results show that the as-cast microstructure of Zn-1.2 wt% Mg zinc alloys with various Bi contents consists of dendritic Zn, eutectic Mg2Zn11, and a core-shell Mg3Bi2/Bi heterostructure. Transmission electron microscopy (TEM) results reveal that rod-like and spherical Mg3Bi2 intermetallics, identified as (Mg1-xZnx)3Bi2 variants with chemical compositions of Mg0.99Zn2.01Bi2 and Mg2.03Zn0.97Bi2, respectively, exhibit a crystallographic relationship between hexagonal structured Mg3Bi2 and hexagonal close-packed Zn matrix: (112¯0)Mg3Bi2//(101¯0)Zn and [112¯0]Mg3Bi2//[0001]Zn. In addition, a possible coexisting orientation relationship of (011¯)Mg2Zn11//(020)Bi is observed at Bi/Mg3Bi2 interface for Mg2Zn11 precipitates. Meanwhile, numerous stripes and subgrains in Mg3Bi2 are discovered to align at precise angles with dislocations, owing to lattice strains induced by substitution of Mg atoms with Zn. Moreover, the simultaneous improvement in strength and ductility of the Zn-1.2 wt% Mg zinc alloy containing 1.5 wt% Bi is predominantly governed by the core-shell morphology and sizes of the Mg3Bi2/Bi heterostructure. The strengthening-toughening mechanism of the core-shell Mg3Bi2 reinforced zinc alloy involves crack deflection and ligament toughening, while also impeding crack propagation through obstacles or crack-bridging behind the crack tip. This mechanism reveals a synergistic effect of soft-shell toughening and hard-core strengthening thereby enhancing cracking resistance of the zinc alloys.

Original languageEnglish
Article number189671
JournalJournal of Alloys and Compounds
Volume1078
DOIs
StatePublished - 25 Jul 2026

Keywords

  • Crack
  • Crystallographic orientation
  • Heterostructure
  • Microstructure
  • Transmission electron microscopy

Fingerprint

Dive into the research topics of 'Microstructural evolution and simultaneous strengthening and toughening of core-shell Mg3Bi2 reinforced Zn-1.2 wt% Mg zinc alloys'. Together they form a unique fingerprint.

Cite this