Microstructural characteristics and low cycle fatigue properties at 230 °C of different weld zone materials from a 100 mm thick dissimilar weld of ultra-supercritical rotor steel

  • Jian Long
  • , Lin Jie Zhang
  • , Qun Bing Zhang
  • , Wen Ke Wang
  • , Jie Zhong
  • , Jian Xun Zhang
  • Xi'an Jiaotong University
  • Xi'an Aeronautical University
  • Dongfang Steam Turbine Limited Company

Research output: Contribution to journal › Article › peer-review

37 Scopus citations

Abstract

The low cycle fatigue properties at 230 °C and the microstructures of the material in different zones of 100-mm thick dissimilar joint made of ultra-supercritical rotor steels were studied. The microstructures, failure path and the fatigue fracture surfaces were characterized by scanning electron microscope and transmission electron microscopy. The relationship between strain level and fatigue life of 30Cr1Mo1V (BM-1), weld-seam (SAW) and 30Cr2Ni4MoV (BM-2) at 230 °C were obtained, respectively. The effects of microstructural characteristics on low cycle fatigue performance at 230 °C were discussed based on the morphology of dislocation cells in fatigued samples.

Original languageEnglish
Article number105248
JournalInternational Journal of Fatigue
Volume130
DOIs
StatePublished - Jan 2020

Keywords

  • CrMo-steel
  • Low cycle fatigue
  • Rotor
  • Thick wall
  • Welded joint

Fingerprint

Dive into the research topics of 'Microstructural characteristics and low cycle fatigue properties at 230 °C of different weld zone materials from a 100 mm thick dissimilar weld of ultra-supercritical rotor steel'. Together they form a unique fingerprint.

Cite this