Abstract
The macroporous SnO2 is prepared using close packed carbonaceous sphere template which synthesized from glucose by hydrothermal method. The structure and morphology of the macroporous SnO2 are evaluated by XRD and FE-SEM. The average pore size of the macroporous SnO2 is about 190 nm and its wall thickness is less than 10 nm. When the macroporous SnO 2 filled with carbon is used as an anode material for lithium-ion battery, the capacity is about 380 mAh g-1 after 70 cycles. The improved cyclability is attributed to the carbon matrix which is used as an effective physical buffer to prevent the collapse of the well dispersed macroporous SnO2.
| Original language | English |
|---|---|
| Pages (from-to) | 5969-5973 |
| Number of pages | 5 |
| Journal | Journal of Alloys and Compounds |
| Volume | 509 |
| Issue number | 20 |
| DOIs | |
| State | Published - 19 May 2011 |
UN SDGs
This output contributes to the following UN Sustainable Development Goals (SDGs)
-
SDG 7 Affordable and Clean Energy
Keywords
- Anode
- Electrochemical property
- Lithium ion battery
- Macroporous
- Tin dioxide
Fingerprint
Dive into the research topics of 'Large-scale synthesis of macroporous SnO2 with/without carbon and their application as anode materials for lithium-ion batteries'. Together they form a unique fingerprint.Cite this
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver