Abstract
In order to improve the sidewall quality of solid parts in laser metal direct forming, the paper focused on the difference of powder quantity actually injected into molten pool at the edge and inner positions when forming the solid parts, and the influence of curvature radius of the solid part's edge on the powder quantity injected into the molten pool at the edge position was also investigated. The result shows that the distance between the cladding point and the solid part's edge seriously affects the powder quantity injected into the molten pool and that the powder quantity injected into the molten pool at the edge positions is about 1.2 times more than that at the inner positions. However, the change of curvature radius of the solid part's edge has little effect on the quantity of powder injected into the molten pool. The sidewall roughness of solid parts can be effectively reduced by increasing the powder feeding rate at the edge positions to about 1.2 times more than that at the inner position. Using this powder compensation method, a tip of turbine blade with the sidewall roughness Ra of 16.2-20.8 μm was fabricated.
| Original language | English |
|---|---|
| Pages (from-to) | 2703-2711 |
| Number of pages | 9 |
| Journal | International Journal of Advanced Manufacturing Technology |
| Volume | 68 |
| Issue number | 9-12 |
| DOIs | |
| State | Published - Oct 2013 |
Keywords
- Laser metal direct forming
- Numerical simulation
- Powder flow
- Sidewall roughness
Fingerprint
Dive into the research topics of 'Influence of powder flow on sidewall quality of solid parts in laser metal direct forming'. Together they form a unique fingerprint.Cite this
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver